GA-6071AHT Silicone Rubber for Ultra-high Voltage Cable (HCR)
Aplikasi: cocog kanggo ngasilake kabel proteksi tegangan dhuwur energi ijo, kabel tahan suhu dhuwur, kabel transit rel, lsp.
Fitur utama: tundhuk karo syarat 1S06722-1: 2011 (E), GB / T33430-2016, lan LV 216; Resistance suhu dhuwur lan rendah sing apik banget, proses ekstrusi sing apik, properti insulasi listrik sing apik; Lulus tes penuaan termal kanggo 3000h, DC lan sistem platedinum.
Tes: platina A: 0,3%, platina B: 1,2%, 130 ℃ x 5 menit.
| KELAS E (180 ℃) Parameter produk | |||
| produk | GA-6071AHT | GA-6071AHTAB | |
| Penampilan | Tembus | ||
| Williamplastisitas | 265 | 265 | |
| Kekerasan (ShoreA) | 65 | 68 | |
| Kapadhetan (g/cm3) | 1.2 | 1.2 | |
| Kekuatan tarik (MPa) | 10 | 10.5 | |
| Elongasi (%) | 450 | 700 | |
| Kekuwatan sobek (kN/m) | 33 | 45 | |
| Resistivitas volume (Ω·cm) | 1.0*1015 | 1.0*1015 | |
| Kekuatan putus (kV/mm) | 25 | 25 | |