GA-6071AHT Silicone Purgamentum pro Ultra alta intentione Cable (HCR)
Applicatio: apta ad producendum viridis industriam altam intentionem, funem munitum, excelsum renitentem funem, ferriviarium transitum, etc.
Clavis lineamenta: obsecundantia cum requisitis 1S06722-1 :2011 (E), GB/T33430-2016, et LV 216; Excelsa et humilis temperaturae resistentia, bonum extrusionprocessability, bonae insulationis bonae; Canus scelerisque pro 3000h, ab utroque DCBP et platinumsystem sanari potest.
Test: platinum A: 0.3%, platinum B: 1.2%, 130℃ x 5min.
| ORDO E(180℃)Product parametris | |||
| Productum | GA-6071AHT | GA-6071AHTAB | |
| Aspectus | Translucens | ||
| Williamplasticity | 265 | 265 | |
| Duritia (ShoreA) | 65 | 68 | |
| Densitas (g/cm3) | 1.2 | 1.2 | |
| Roboris distrahentes (MPa) | 10 | 10.5 | |
| Prolongatio(%) | 450 | 700 | |
| Robur scindere (kN/m) | 33 | 45 | |
| Volumen resistivity (Ω·cm) | 1.0*1015 | 1.0*1015 | |
| Confringe vires (kV/mm) | 25 | 25 | |