GA-6071AHT Silicone Rabara bakeng sa Ultra-phahameng gagamalo Cable (HCR)
Kopo: loketseng bakeng sa hlahisa tala matla gagamalo phahameng shielded thapo, hightemperature-mahanyetsa kabel, seporo transit thapo, joalo-joalo.
Litšobotsi tse senotlolo: lumellana le ditlhoko tsa 1S06722-1 :2011 (E), GB / T33430-2016, le LV 216;Excellent phahameng le tlaase temperatureresistance, molemo extrusionprocessability,goodelectrical kwahelang thepa;Fesa teko ea mogote botsofali bakeng sa 3000h, ka fodisoa ke bobeli DCBP le platinumsystem.
Teko: polatinamo A: 0.3%, polatinamo B: 1.2%, 130 ° C x 5min.
| CLASS E (180°C)Ditekanyetos sehlahiswa | |||
| Setšweletšwa | GA-6071AHT ya go dira bjalo | GA-6071AHTAB ya go swana le yona | |
| Ponagalo | Translucent . | ||
| Williamplasticity . | 265 | 265 | |
| Go thatafala (Sorea) . | 65 | 68 | |
| Kitlano (G / CM3) . | 1.2 | 1.2 | |
| Matla a go goga (MPA) . | 10 | 10.5 | |
| go telefa (%) . | 450 | 700 | |
| Matla a Meokgo (KN/M) . | 33 | 45 | |
| Bophahamo ba modumo resistivity (Ω · cm) . | 1.0 * 10 e 10.015 | 1.0 * 10 e 10.015 | |
| Kgaola matla (kV / mm) . | 25 | 25 | |