GA-6071AHT
Herchy
| Wiwa: | |
|---|---|
| Opoiye: | |
GA-6071AHT Roba Silikoni fun Okun Foliteji Ultra-giga (HCR)
Ohun elo: o dara fun iṣelọpọ agbara alawọ ewe giga foliteji idabobo okun, okun ti o ni iwọn otutu, okun irekọja ọkọ oju-irin, bbl
Key awọn ẹya ara ẹrọ: ni ibamu pẹlu awọn ibeere ti 1S06722-1: 2011 (E), GB / T33430-2016, ati LV 216; O tayọ ga ati kekere otutu resistance, ti o dara extrusionprocessability, goodelectrical idabobo ohun ini; Kọja awọn igbeyewo ti gbona ti ogbo fun 3000h, DC le curtin.
Idanwo: Pilatnomu A: 0.3%, Pilatnomu B: 1.2%, 130℃ x 5min.
| CLASS E(180℃) Awọn paramita ọja | |||
| Ọja | GA-6071AHT | GA-6071AHTAB | |
| Ifarahan | Translucent | ||
| Williamplasticity | 265 | 265 | |
| Lile ( ShoreA) | 65 | 68 | |
| Ìwúwo (g/cm3) | 1.2 | 1.2 | |
| Agbara fifẹ (MPa) | 10 | 10.5 | |
| Ilọsiwaju(%) | 450 | 700 | |
| Agbara omije (kN/m) | 33 | 45 | |
| Atako iwọn didun (Ω·cm) | 1.0*1015 | 1.0*1015 | |
| Pipin agbara (kV/mm) | 25 | 25 | |