Kawotchou silikon GA-6071AHT pou kab vòltaj ultra-wo (HCR)

Kawotchou silikon GA-6071AHT pou kab vòltaj ultra-wo (HCR)
Aplikasyon: apwopriye pou pwodwi enèji vèt segondè vòltaj pwoteje kab, hightemperature ki reziste kab, kab transpò tren, elatriye.
Karakteristik kle: konfòme ak egzijans 1S06722-1: 2011 (E), GB/T33430-2016, ak LV 216; Ekselan rezistans tanperati wo ak ba, bon extrusionprocessability, bon pwopriyete izolasyon elektrik; Pase tès la nan aje tèmik pou 3000h sistèm DCBP ak platinum ka tou de.
  • GA-6071AHT

  • Herchy

Disponibilite:
Kantite:

Kawotchou silikon GA-6071AHT pou kab vòltaj ultra-wo (HCR)


Aplikasyon: apwopriye pou pwodwi enèji vèt segondè vòltaj pwoteje kab, hightemperature ki reziste kab, kab transpò tren, elatriye.

Karakteristik kle: konfòme ak kondisyon ki nan 1S06722-1: 2011 (E), GB/T33430-2016, ak LV 216; Ekselan rezistans tanperati wo ak ba, bon extrusionprocessability, bon pwopriyete izolasyon elektrik; Pase tès la nan aje tèmik pou 3000h ak platinum DCBP tou de.

Tès: platinum A: 0.3%, platinum B: 1.2%, 130℃ x 5min.


KLAS E (180 ℃) Paramèt pwodwi
Pwodwi GA-6071AHT GA-6071AHTAB
Aparans Translusid
Williamplasticity 265 265
Dite (ShoreA) 65 68
Dansite (g/cm3) 1.2 1.2
Fòs rupture (MPa) 10 10.5
elongasyon (%) 450 700
Fòs chire (kN/m) 33 45

Volim rezistans (Ω·cm) 1.0 * 1015 1.0 * 1015

Kraze fòs (kV/mm) 25 25


Previous: 
Pwochen: 

Lyen RAPID

PWODWI NOU YO

ENFÒMASYON KONTAK

Add: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Dwa     2023 Shanghai Herchy Rubber co, Ltd. Sitemap |   Règleman sou enfòmasyon prive | Sipòte By Leadong.