Color: black
Vulcanization system: bisphenol system
Fluorine content: 68%
Hardness: 70±5 SHORE A
Mooney viscosity: ML(1+10)121℃ 30-50
Size specification: can be more customized (sheet)
Vulcanization condition: 175℃*10min Secondary vulcanization: 200℃*4h (2mm standard test piece)
Minimum order quantity: 50kg
This product has good flame retardancy, meet UL94/FV 0 flame retardant level. Excellent oil resistance, solvent resistance, high and low temperature resistance
Application: suitable for producing silicone human mask, silicone artificialorgans, silicone models, and high simulation mold of candy fruit, chocolate,biscuits, cakes etc.
Key features: good fluidity, easily debubbling