GA-2040 LSR for Cable Accessories (LSR)
Product description:one kind of high voltage-resistant liquid silicone rubber of two componentcatalyzed by platinum complex, the A/B ratio as 1 :1, component A and B 1s transparent and grey,respectively.
Application: intermediate voltage cable accessories, internal and external cold shrink terminal,transition joint,sheath.
Key features:injection molding, high tensile, high elongation, high tear strength,small fix tensionset, fast curing speed, pass the authentication of RoHS and REACH.