Maybe you are a Ethylene Propylene Diene Rubber purchasing manager, who are looking for high quality Ethylene Propylene Diene Rubber, and Herchy are a professional manufacturer & supplier that can meet your needs. Not only Ethylene Propylene Diene Rubber we produced have certificated the international industry standard, but we can also meet your customization needs. We provide online, timely service and you can get professional guidance on Ethylene Propylene Diene Rubber. Don't hesitate to get in touch with us if you are interested in Ethylene Propylene Diene Rubber, we won't let you down.
Appearance and condition: Beige or pale yellow blocky Third monomer type and content: ENB, 5.5% Ethylene content: 69.5% Mooney viscosity: ML(1+4)125°C 80 Size: 25kg/block MOQ: 25kg Packing: boxed
Appearance and condition: Beige or pale yellow blocky Third monomer type and content: ENB, 4.5% Ethylene content: 55.5% Mooney viscosity: ML(1+4)125°C 55 Size: 25kg/block MOQ: 25kg Packing: boxed
Appearance and condition: Beige or pale yellow blocky Third monomer type and content: ENB, 8.5% Ethylene content: 52.5% Mooney viscosity: ML(1+4)125°C 68 Oil content:20% Size: 25kg/block MOQ: 25kg Packing: boxed
Appearance and condition: Beige or pale yellow blocky Third monomer type and content: ENB, 4% Ethylene content: 61% Mooney viscosity: ML(1+4)100°C 44 Size: 25kg/block MOQ: 25kg Packing: boxed