For SUPRENE, everyone has different special concerns about it, and what we do is to maximize the product requirements of each customer, so the quality of our SUPRENE has been well received by many customers and enjoyed a good reputation in many countries. Herchy SUPRENE have characteristic design & practical performance & competitive price, for more information on the SUPRENE, please feel free to contact us.
Appearance and condition: white (transparent or translucent) blocky Third monomer type and content: ENB, 8.5% Ethylene content: 72% Oil content:100% Mooney viscosity: ML(1+4)125°C 47 Size: 25kg/block MOQ: 25kg Packing: boxed
Appearance and condition: white (transparent or translucent) blocky Third monomer type and content: ENB, 5.7% Ethylene content: 58% Mooney viscosity: ML(1+4)125°C 84 Size: 25kg/block MOQ: 25kg Packing: boxed
Appearance and condition: white (transparent or translucent) blocky Third monomer type and content: ENB, 9.4% Ethylene content: 55% Mooney viscosity: ML(1+4)125°C 29 Size: 25kg/block MOQ: 25kg Packing: boxed
Appearance and condition: white (transparent or translucent) blocky Third monomer type and content: ENB, 4.7% Ethylene content: 70% Oil content:75% Mooney viscosity: ML(1+4)125°C 62 Size: 25kg/block MOQ: 25kg Packing: boxed
Appearance and condition: white (transparent or translucent) blocky Third monomer type and content: ENB, 4.1% Ethylene content: 58% Mooney viscosity: ML(1+4)125°C 84 Size: 25kg/block MOQ: 25kg Packing: boxed
Appearance and condition: white (transparent or translucent) blocky Third monomer type and content: ENB, 5.7% Ethylene content: 71% Mooney viscosity: ML(1+4)125°C 24 Size: 25kg/block MOQ: 25kg Packing: boxed