Imikhiqizo yenjoloba eyigwebu ikhiqizwa ngendlela yerabha engokoqobo noma yamakhemikhali enerabha njengesisekelo sokuthola imikhiqizo yesakhiwo esinezimbotshana zenjoloba enjengesipontshi. Lobu buchwepheshe busetshenziswe kabanzi ezimbonini ezihlukahlukene zokukhiqiza, ezifana neminyango yezimoto kanye nezimpawu zamafasitela, ama-cushioning pads, ama-gaskets wokwakha izakhiwo, izinto zokuzamazama komhlaba, izikhungo zokuvikela ezemidlalo, njll.

橡胶脱模.png
Izinto ezithinta ukudilizwa kwemikhiqizo yenjoloba kanye nezinyathelo zokuphikisa

Ngokuvamile, imikhiqizo ebunjwe ngenjoloba kufanele ibunjwe ngokusebenzisa isikhunta esihambisanayo sokucubungula ukubunjwa, umkhiqizo wenjoloba ngemuva kokushisa okuphezulu, ukuvuvuka kwengcindezi ephezulu, kusukela emgodini wokubumba noma umgogodla wesikhunta owaziwa ngokuthi ukukhululwa kwesikhunta. Ukudilizwa kabi kungesinye sezizathu ezibalulekile zokukhubazeka kwekhwalithi yemikhiqizo yenjoloba kanye nomthelela ekusebenzeni kahle kokukhiqiza. Kungabangela ukukhubazeka okunjengokuhlanekezela nokuklebhuka kwezingxenye, futhi okunye konakalise isikhunta, kulethe inkinga ekukhiqizeni okuvamile. Ukutadisha izici ezingezinhle ezithinta ukubhidlizwa kwemikhiqizo yenjoloba kubaluleke kakhulu ukuze kuqinisekiswe ikhwalithi yemikhiqizo, ukuvimbela amaphutha, ukuvimbela ukulahlwa, kanye nokwenza ngcono ukusebenza kahle kokukhiqiza.

455cd9598e829d34ea85719d0552a8a4_副本.jpg
Izinkinga ezijwayelekile zekhwalithi nezisombululo kugwebu lwenjoloba

Izinkinga ezijwayelekile zekhwalithi nezisombululo kugwayi wenjoloba 1、Izimbobo ezinegwebu ezinganele 2. Isikhunta esinganele sokugcwalisa 3. Izimbobo ezinegwebu ezingalingani (ezinkulu kakhulu noma ezincane kakhulu) 4. ukuvuvuka ngokweqile noma ukuvuvuka

1122.png
Ukuhlaziywa kwezimbangela zemiphetho ephukayo nemangelengele yemikhiqizo yenjoloba

Imikhiqizo eminingi yenjoloba iyabunjwa, futhi ngemva kokubunjwa, i-vulcanization ukuthola imikhiqizo enezakhiwo ezifanelekayo zomzimba, ukubukeka komkhiqizo akunawo amaphutha amakhulu, kodwa indlela evamile yokusika ayikwazi ukulungisa izidingo zokubukeka komkhiqizo, kukhona ama-burrs amancane angeke asuswe, ukulungiswa kwezandla noma ukuchithwa kubangela ukuchithwa kwezomnotho okuningi. Ngalesi sikhathi, ukwakheka kwesakhiwo somugqa wokubumba isikhunta somkhiqizo kubaluleke kakhulu, indlela yokuklama udebe, umugqa wokuchichima kanye ne-groove echichimayo, njll., ngeke kuchazwe lapha, ungabhekisela ku-'Rubber Mold Design Manual'. Ukugxila kwalesi sihloko ukuchaza kusukela kufomula kanye nenqubo, ngoba isikhunta ngokuvamile siklanywe asikwazi ukuguqula noma ukulahla isikhunta (imfucumfucu yezomnotho), ngokuvamile sithola unjiniyela wefomula ukuze aguqule ifomula noma aguqule inqubo ukuze kuzuzwe ukudabuka kalula.

IZIXHUMANISI EZISHESHAYO

IMIKHIQIZO YETHU

ULWAZI LOKUXHUMANA

Engeza: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Ucingo / WhatsApp / Skype: +86 15221953351
I-imeyili:  info@herchyrubber.com
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Imephu yesayithi |   Inqubomgomo Yobumfihlo | Sekela Ngu I-Leadong.