Kev daws

Koj tseem nyob ntawm no: Tsev » Kev daws teeb meem » Kev daws teeb meem
发泡胶.jpg ib
foamed roj hmab

Cov khoom siv roj hmab ua npuas ncauj yog tsim los ntawm lub cev lossis tshuaj foaming txoj kev nrog roj hmab ua cov khoom siv hauv paus kom tau txais cov ntaub so ntswg zoo li roj hmab ntxeem tau cov qauv khoom. Cov cuab yeej no tau siv dav hauv ntau qhov kev lag luam, xws li tsheb qhov rooj thiab qhov rai ntsaws ruaj ruaj, cushioning pads, lub tsev siv gaskets, seismic cov ntaub ntawv, cov chaw tiv thaiv kev ua si, thiab lwm yam.

橡胶脱模.png
Cov yam ntxwv cuam tshuam rau demolding ntawm cov khoom siv roj hmab thiab kev tiv thaiv

Feem ntau hais lus, cov khoom siv roj hmab molded yuav tsum tau molded los ntawm cov pwm sib thooj rau molding ua, cov khoom siv roj hmab tom qab kub siab, siab siab vulcanization, los ntawm pwm kab noj hniav los yog pwm core feem ntau hu ua pwm tso tawm. Tsis zoo demolding yog ib qho ntawm cov laj thawj tseem ceeb rau qhov tsis zoo ntawm cov khoom siv roj hmab thiab cuam tshuam rau kev tsim khoom. Nws tuaj yeem ua rau muaj qhov tsis xws luag xws li distortion thiab tearing ntawm qhov chaw, thiab qee qhov kev puas tsuaj rau pwm, ua rau muaj teeb meem rau kev tsim khoom. Kawm txog cov yam tsis zoo uas cuam tshuam rau kev demolding ntawm cov khoom siv roj hmab yog qhov tseem ceeb los xyuas kom meej cov khoom zoo, tiv thaiv qhov tsis xws luag, tiv thaiv cov khoom seem, thiab txhim kho kev tsim khoom.

455cd9598e829d34ea85719d0552a8a4_副本.jpg
Cov teeb meem zoo thiab cov kev daws teeb meem hauv cov roj hmab foaming

Cov teeb meem zoo thiab cov kev daws teeb meem hauv cov roj hmab foaming 1 、 Tsis txaus foaming qhov 2. Tsis txaus filling pwm 3. Qhov tsis sib xws foaming (loj lossis me dhau) 4. over-vulcanization lossis under-vulcanization

1 122.png
Kev soj ntsuam ntawm qhov ua rau brittle thiab jagged npoo ntawm cov khoom siv roj hmab

Ntau cov khoom siv roj hmab yog molded, thiab tom qab molding, vulcanization kom tau cov khoom uas tsim nyog lub cev muaj zog, cov tsos ntawm cov khoom tsis muaj qhov tsis xws luag, tab sis cov pa trimming txoj kev tsis tuaj yeem kho cov kev xav tau ntawm cov khoom, muaj cov burrs me me tsis tuaj yeem raug tshem tawm, phau ntawv kho lossis scrapping ua rau muaj kev lag luam pov tseg ntau. Lub sijhawm no, kev tsim qauv ntawm cov pwm clamping kab ntawm cov khoom yog qhov tseem ceeb tshwj xeeb, yuav ua li cas los tsim daim di ncauj, hla kab thiab dhau qhov zawj, thiab lwm yam, yuav tsis tau piav qhia ntawm no, koj tuaj yeem xa mus rau 'Rubber Pwm Design Manual'. Lub hom phiaj ntawm tsab xov xwm no yog piav qhia los ntawm cov qauv thiab cov txheej txheem, vim tias cov pwm feem ntau tsim tsis tuaj yeem hloov kho lossis khawb cov pwm (kev lag luam pov tseg), feem ntau nrhiav ib tus kws tsim qauv los hloov cov qauv los yog hloov cov txheej txheem kom ua tau yooj yim tearing.

QUICK LINKS

Peb cov khoom

Tiv tauj xov xwm

Ntxiv: No.33, Txoj Kev 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Daim duab qhia chaw |   Txoj Cai Tswjfwm Ntiag Tug | Txhawb nqa By Leadong.