Appearance and condition: white (transparent or translucent) blocky Third monomer type and content: ENB, 4% Ethylene content: 68.5% Mooney viscosity: ML (1+4) 125°C 70 Size: 25kg/bag MOQ: 25kg Packing: boxed
Appearance and condition: white (transparent or translucent) granular Third monomer type and content: ENB, 4% Ethylene content: 68.5% Mooney viscosity: ML (1+4) 125°C 70 Size: 25kg/bag MOQ: 25kg Packing: boxed
Appearance and condition: white (transparent or translucent) blocky Third monomer type and content: ENB, 4.6% Ethylene content: 57.2% Oil charge: 20% Mooney viscosity: ML (1+4) 125°C 60 Size: 25kg/bag MOQ: 25kg Packing: boxed
Appearance and condition: Beige or pale yellow blocky Third monomer type and content: ENB, 4.5% Ethylene content: 59.5% Mooney viscosity: ML(1+4)125°C 47 Oil content:10% Size: 25kg/block MOQ: 25kg Packing: boxed