Bayyanawa da yanayin: fari (m ko mai bayyanawa) toshe
Nau'in monomer na uku da abun ciki: ENB, 4%
abun ciki na Ethylene: 68.5%
Dankowar Mooney: ML (1 + 4) 125 ° C 70
Girman: 25kg / jaka
MOQ: 25kg
Packing: akwati
Bayyanawa da yanayin: fari (m ko mai bayyanawa) toshe
Nau'in monomer na uku da abun ciki: ENB, 4.6%
abun ciki na Ethylene: 57.2%
cajin mai: 20%
dankowar Mooney: ML (1 + 4) 125 ° C 60
Girman: 25kg / jaka
: 25kg
MOQ
Bayyanar da yanayin: fari (m ko m)
abun ciki na Ethylene toshe: 55%
abun ciki na propylene: 45%
Mooney danko: ML (1 + 4) 100 ° C 33
Girman: 25kg / jaka
MOQ: 25kg
Shiryawa: akwati