Ponagalo le maemo: tšoeu (e bonaletsang kapa translucent) granular
Mofuta oa boraro oa monomer le dikahare: ENB, 4%
Diteng tsa Ethylene: 68.5%
Viscosity ea mooney: ML (1+4) 125 ° C 70
Boholo: 25kg / mokotla
MOQ: 25kg
Packing: boxed
Ponagalo le maemo: tšoeu (e bonaletsang kapa translucent) blocky
Mofuta oa boraro oa monomer le dikahare: ENB, 4.6%
Diteng tsa ethylene: 57.2%
Tefiso ea oli: 20%
Viscosity ea mooney: ML (1+4) 125°C 60
Boholo: 25kg/mokotla
MOQ: 25kg
Packing: boxed