A rilru a buai em em a, a rilru a hah em em bawk a.
A lan dan leh a awm dan: White (Transparent or Translucent) Granular
Third Monomer chi leh Thupui: ENB, 4%
Ethylene awm zat: 68.5%
Mooney Viscosity: ML (1+4) 125°C 70
Size: 25KG/BAG
MOQ: 25KG
Packing: Boxed