| Ọja sile | |||||||
| Ọja | GA-9930 | GA-9935H | GA-9935 | GA-9940 | GA-9950 | GA-9960 | GA-9970T |
| Ifarahan | Translucent | Milky White | Translucent | ||||
| Williamplasticity | 120 | 140 | 130 | 140 | 160 | 200 | 250 |
| Lile ( ShoreA) | 30 | 33 | 36 | 40 | 50 | 60 | 70 |
| Ìwúwo (g/cm3) | 1.1 | 1.1 | 1.1 | 1.11 | 1.12 | 1.15 | 1.17 |
| Agbara fifẹ (MPa) | 7 | 9.5 | 9.5 | 8 | 9 | 9 | 9.5 |
| Ilọsiwaju(%) | 700 | 800 | 700 | 600 | 400 | 300 | 250 |
| Agbara omije (kN/m) | 15 | 15 | 15 | 15 | 20 | 20 | 20 |
| 175 'C x22h Funmorawon(%) | 15 | 20 | 15 | 15 | 15 | 15 | 15 |