Herchy is
Ethylene Propylene Diene Rubber manufacturers and suppliers in China who can wholesale
Ethylene Propylene Diene Rubber. We can provide professional service and better price for you. If you interested in
Ethylene Propylene Diene Rubber products, please contact with us. Tips: Special needs, for example: OEM, ODM, customized according to demands, design and others, please email us and tell us detail needs. We follow the quality of rest assured that the price of conscience, dedicated service.
Appearance and condition: Beige or pale yellow blocky
Third monomer type and content: ENB, 4.4%
Ethylene content: 68.6%
Mooney viscosity: ML(1+4)125°C 77
Size: 25kg/block
MOQ: 25kg
Packing: boxed
Appearance and condition: Beige or pale yellow blocky
Third monomer type and content: ENB, 4.5%
Ethylene content: 59.5%
Mooney viscosity: ML(1+4)125°C 47
Oil content:10%
Size: 25kg/block
MOQ: 25kg
Packing: boxed
Appearance and condition: Beige or pale yellow blocky
Third monomer type and content: ENB, 4.4%
Ethylene content: 68.6%
Mooney viscosity: ML(1+4)125°C 60
Size: 25kg/block
MOQ: 25kg
Packing: boxed
Appearance and condition: Beige or pale yellow blocky
Third monomer type and content: ENB, 8.9%
Ethylene content: 60.1%
Mooney viscosity: ML(1+4)100°C 64
Size: 25kg/block
MOQ: 25kg
Packing: boxed