GA-99XX
Herchy
| kasedhiyan: | |
|---|---|
| Jumlah: | |
GA-99XX Vapor Phase Silica Reinforcing Low Compression Set Silicone Rubber (HCR)
Aplikasi: cocok kanggo produksi ring sealing, cots, auto parts lan produk liyane.
Fitur utama: daya tahan dhuwur, set kompresi sithik, HSE ora beracun, lulus otentikasi RoHS, REACH lan FDA.
Tes: 1% agen curing (50% tempel DBPMH ing permen karet silikon), 175心5minx 15MPa.
| Parameter produk | |||||||
| produk | GA-9930 | GA-9935H | GA-9935 | GA-9940 | GA-9950 | GA-9960 | GA-9970T |
| Penampilan | Tembus | Putih Susu | Tembus | ||||
| Williamplastisitas | 120 | 140 | 130 | 140 | 160 | 200 | 250 |
| Kekerasan (ShoreA) | 30 | 33 | 36 | 40 | 50 | 60 | 70 |
| Kapadhetan (g/cm3) | 1.1 | 1.1 | 1.1 | 1.11 | 1.12 | 1.15 | 1.17 |
| Kekuatan tarik (MPa) | 7 | 9.5 | 9.5 | 8 | 9 | 9 | 9.5 |
| Elongasi (%) | 700 | 800 | 700 | 600 | 400 | 300 | 250 |
| Kekuwatan sobek (kN/m) | 15 | 15 | 15 | 15 | 20 | 20 | 20 |
| 175'C x22h Kompresi(%) | 15 | 20 | 15 | 15 | 15 | 15 | 15 |