High Hardness, High Wear Resistance, HNBR ma Injection Ne Oilfield

High-Performance HNBR for Injection Molding & Oilfield Applications

Yɛn High Hardness, High Wear-Resistance HNBR yɛ engineered ma ahwehwɛde oilfield ne mfiridwuma tebea horow, a ɛka mfiridwuma su soronko ne nnuru a ɛkorɔn a ɛko tia bom. Wɔayɛ no sɛ wɔmfa nwene nneɛma a wɔde twitwiw nneɛma mu, na hydrogenated nitrile butadiene rɔba (HNBR) a ɛkɔ akyiri yi ma ɛtra hɔ kyɛ a ɛso bi nni wɔ tebea horow a emu yɛ den mu, a nea ɛka ho ne nhyɛso kɛse a wɔde tu fam, adwuma a wɔyɛ wɔ tokuru ase, ne mfiri a wɔde yɛ pɛtro.
 
  • HNBR8501 na ɛwɔ hɔ

  • HERCHY na ɔkyerɛwee

Nea ɛwɔ hɔ:
Dodoɔ:

High Hardness, High Wear Resistance, HNBR ma Injection Ne Oilfield



Yɛn High Hardness, High Wear-Resistance HNBR yɛ engineered ma ahwehwɛde oilfield ne mfiridwuma tebea horow, a ɛka mfiridwuma su soronko ne nnuru a ɛkorɔn a ɛko tia bom. Wɔayɛ no sɛ wɔmfa nwene nneɛma a wɔde twitwiw nneɛma mu, na hydrogenated nitrile butadiene rɔba (HNBR) a ɛkɔ akyiri yi ma ɛtra hɔ kyɛ a ɛso bi nni wɔ tebea horow a emu yɛ den mu, a nea ɛka ho ne nhyɛso kɛse a wɔde tu fam, adwuma a wɔyɛ wɔ tokuru ase, ne mfiri a wɔde yɛ pɛtro.



Nneɛma Titiriw a Ɛwɔ Hɔ:  

- Hardness: [85Shore A Hardness , 70-90 Shore A] – Wɔayɛ no yie ama rigidity ne impact resistance.

- Tensile Strength: [29.79MPa, ≥20 MPa] – Ɛhwɛ sɛ structure mudi mu kura wɔ adesoa a emu yɛ duru ase.

- Elongation at Break: [383%, 200-400%] – Ɛkari pɛ wɔ nsakraeɛ ne nusuo a ɛko tia a ɛkorɔn.

- Mooney Viscosity: [55, ML(1+4) 30-60] – Ɛyɛ papa ma pɛpɛɛpɛ injection molding a ɛyɛ den afã horow.

- Abrasion Resistance: Ɛboro nnwuma gyinapɛn so (wɔasɔ ahwɛ sɛnea ASTM D5963/DIN 53516 te), eye ma drilling nnwinnade, seals, ne mfiri a ɛda abrasive media adi.



Adwumayɛ mu Nsɛntitiriw:  

- Oil & Chemical Resistance: Ɛgyina ngo a ɛyɛ den, nsuo a wɔde tu fam, ne acidic/alkaline tebea ano.

- Thermal Stability: Ɛyɛ adwuma a wotumi de ho to so wɔ ɔhyew a efi -30°C kosi +150°C (-22°F kosi +302°F).

- Wear Resistance: Engineered ma adwumayɛ a ɛtra hɔ kyɛ wɔ high-friction applications te sɛ pump seals, valve components, ne downhole mfiri.



Nnwuma a Wɔde Di Dwuma:  

- Oilfield Nnwinnade: Nsɔano, gaskets, blowout preventers, ne drilling adwinnade afã horow.

- Injection-Molded Afã horow: Customizable ma petrochemical valves, mfiri afã horow, ne wear-resistant liners.

- Nneɛma a Atwa Yɛn Ho Ahyia a Ɛyɛ Den: Ɛfata ma nsuo a ɛwɔ abura mu tebea a ɛyɛ den, ɔhyew a ɛkorɔn (HPHT).



Dɛn Nti na Yɛpaw Yɛn HNBR?  

- Precision Molding: Compatible ne automated injection akwan ma ɛka-ahoɔden mass production.

- Extended Service Life: Ɛtew bere a wɔde yɛ adwuma ne nsiesie ho ka wɔ ngo adwumayɛbea adwumayɛ a ɛho hia mu.

- a wɔagye atom sɛ ɛyɛ papa: Ɛne API, ISO, ne NORSOK gyinapɛn ahorow hyia.


[Customizable formulations available – Di yɛn ho nkɔmmɔ na woanya mfiridwuma ho datasheets ne ano aduru a wɔahyɛ da ayɛ.]

Dada: 
Deɛ ɛdi hɔ: 

NKYERƐKYERƐMU A ƐYƐ NTƐM

NKYERƐKYERƐMU A ƐFA NKYERƐKYERƐMU HO

Fa ka ho: No.33, Ɔkwan 159, Taiye Kwan, Fengxian Mantam, Shanghai
Tɛlɛ / WhatsApp / Skype: +86 15221953351 wobɛtumi akyerɛw wo din
Nneɛma a wɔde yɛ adwuma     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap a Wɔde Di Dwuma |   Kokoam Nsɛm Ho Nhyehyɛe | Mmoa a Wɔde Ma Leadong na ɛwɔ hɔ.