Mtengo wa HNBR8501
HERCHY
| kupezeka: | |
|---|---|
| Kuchuluka: | |
Kulimba Kwambiri, Kukaniza Kuvala Kwapamwamba, HNBR ya Jekiseni Ndi Oilfield
Kuuma Kwathu Kwakukulu, Kulimbana Kwambiri Kwambiri HNBR idapangidwa kuti ikhale yofunikira malo opangira mafuta ndi mafakitale, kuphatikiza zida zapadera zamakina ndi kukana kwamphamvu kwamankhwala. Zopangidwira njira zopangira jakisoni, mphira wapamwamba wa hydrogenated nitrile butadiene (HNBR) umapereka kukhazikika kosayerekezeka m'mikhalidwe yovuta kwambiri, kuphatikiza kubowola mwamphamvu, kutsitsa pansi, ndi zida za petrochemical.
Katundu Waukulu:
- Kulimba: [85Shore A Hardness, 70-90 Shore A] - Yokometsedwa chifukwa cha kuuma komanso kukana mphamvu.
- Kulimbitsa Mphamvu: [29.79MPa, ≥20 MPa] - Imatsimikizira kukhulupirika kwadongosolo pansi pa katundu wolemetsa.
- Elongation at Break: [383%, 200-400%] - Kusinthasintha kusinthasintha ndi kukana kwambiri misozi.
- Viscosity ya Mooney: [55, ML (1+4) 30-60] - Yoyenera kupangidwira molondola jekeseni wa zigawo zovuta.
- Kukaniza kwa Abrasion: Kupitilira miyezo yamakampani (yoyesedwa pa ASTM D5963/DIN 53516), yabwino pazida zoboola, zosindikizira, ndi makina omwe amawonetsedwa ndi media abrasive.
Zowonetsa Kachitidwe:
- Kukaniza kwa Mafuta & Chemical: Kulimbana ndi mafuta owopsa, madzi obowola, komanso malo okhala ndi acidic / alkaline.
- Kukhazikika kwa Matenthedwe: Imagwira ntchito modalirika pakutentha koyambira -30°C mpaka +150°C (-22°F mpaka +302°F).
- Wear Resistance: Amapangidwira kuti azigwira ntchito kwanthawi yayitali pamakina okwera kwambiri ngati zisindikizo za pampu, zida za valve, ndi zida zotsitsa pansi.
Mapulogalamu:
- Zida za Oilfield: Zisindikizo, ma gaskets, zoletsa kuphulika, ndi zida zobowola.
- Magawo Opangidwa ndi Jakisoni: Osinthika mwamakonda a mavavu a petrochemical, zida zamakina, ndi zomangira zosavala.
- Malo Owopsa: Oyenera kutengera kuthamanga kwambiri, kutentha kwambiri (HPHT).
Chifukwa Chiyani Sankhani HNBR Yathu?
- Precision Molding: Imagwirizana ndi ma jakisoni odzipangira okha kuti apange misa yotsika mtengo.
- Moyo Wowonjezera Wautumiki: Amachepetsa nthawi yocheperako komanso mtengo wokonza pamachitidwe ofunikira amafuta.
- Ubwino Wotsimikizika: Umagwirizana ndi miyezo ya API, ISO, ndi NORSOK.
[Mapangidwe osinthika omwe alipo - Lumikizanani nafe kuti mumve zambiri zaukadaulo ndi mayankho ogwirizana.]