GA-33 × 1 ke rabara ea silicone e bonaletsang haholo e entsoeng ka silika e tukang, e etselitsoeng ka ho khetheha lits'ebetso tse hlokang ponaletso e phahameng, ho tenyetseha le botsitso. Sehlahisoa sena se loketse ho sebelisoa liindastering tse kang likoloi, lisebelisoa tsa elektroniki, lisebelisoa tsa bongaka, le lisebelisoa tse ling tse sebetsang hantle haholo. E kopanya melemo ea ho hlaka ha optical le thepa e ikhethang ea mechine.
Joaloka moetsi ea ka sehloohong oa rabara ea silicone, re fana ka tharollo e ikhethileng bakeng sa litlhoko tsa hau tsa khoebo. GA-33 × 1 silicone rabara e fumaneha ka limaraka tse fapaneng ho lumellana le litlhoko tsa hau hantle. Hore na o hloka elasticity e phahameng kapa matla a matla a ho taboha, re ka lokisa sebopeho ho fihlela litlhoko tsa hau tse ikhethang. Re ikemiselitse ho fana ka litharollo tsa B2B ka litšebeletso tse ntle tsa bareki le linako tsa phano e potlakileng.
Rabara ea silicone ea GA-33 × 1 e fana ka phetisetso e phahameng, e etsa hore e be e loketseng litiiso, likhase, likarolo tsa bongaka le likarolo tse bōpiloeng tse pepeneneng. E kopana le maemo a thata a indasteri, ho netefatsa boleng le ts'ebetso bakeng sa lits'ebetso tsa bohlokoa moo ts'ebetso le botle bo botle li leng bohlokoa.
Rabara ea rona ea silicone e fana ka matla a makatsang, ho lelefatsa le ho hanyetsa meokho, e netefatsa ts'ebetso e tšoarellang le maemong a khatello e matla. Ka ho hanyetsa mocheso o phahameng, boitsebiso bona bo loketse ho sebelisoa libakeng tse phahameng tsa mocheso. E nepahetse haholo bakeng sa likarolo tsa koloi, lisebelisoa tsa elektroniki le lisebelisoa tsa bongaka tse hlokang ho tšoarella le ho fetoha habonolo.
Teko: 1% ea moemeli oa phekolo (50% peista ea DBPMH ka silicone gum), 175 ° x 5min x 15MPa.
| Lihlahisoa tsa lihlahisoa | |||||
| Sehlahisoa | GA-3331 |
GA-3341 | GA-3351 | GA-3361 | GA-3371 |
| Ponahalo | Tse pepeneneng | ||||
| Williamplasticity |
155 |
200 |
220 |
260 |
280 |
| Ho thatafala (LebopoA) |
30 |
40 |
50 |
60 |
70 |
| Boima ba 'mele(g/cm3) | 1.08 |
1.11 |
1.14 |
1.17 |
1.20 |
| Tensile Matla (MPa) |
9 |
10 |
10 |
10 |
9 |
| Elongation(%) | 850 |
750 |
650 |
550 |
400 |
| Matla a ho lla (kN/m) | 20 |
22 |
25 |
30 |
25 |
| Phetiso(%) |
85 |
86 |
87 |
87 |
88 |
GA-33 × 1 Highly Transparent Silicone Rubber (Fumed Silica) (HCR) ke thepa e fapaneng e etselitsoeng mefuta e mengata ea lisebelisoa. Ponaletso ea eona e phahameng, matla a phahameng a ho taboha, le ho hanyetsa mocheso li etsa hore e be sebaka se loketseng liindasteri tse hlokang ho ts'epahala, joalo ka likoloi, lisebelisoa tsa elektroniki le lisebelisoa tsa bongaka. Re fana ka litharollo tsa moetlo ho fihlela litlhoko tse ikhethileng tsa sehlahisoa, ho netefatsa ts'ebetso e ntle haholo le ho tšoarella lits'ebetsong tse fapaneng. Joaloka moetsi ea tšepahalang oa rabara ea silicone, re fana ka lihlahisoa tsa boleng bo holimo, tse bolokang chelete e ngata ho latela litlhoko tsa hau.

GA-33 × 1 rabara ea silicone e etselitsoe pepeneneng e phahameng, e etsa hore e be e loketseng lihlahisoa tse hlakileng tsa rabara tsa silicone. Boitsebiso bona bo loketse lintho tse kang li-pacifiers, litiiso tse bonaletsang, le likarolo tse ling tse hlakileng tsa rabara moo ho hlakileng le matla a hlokahalang. Hore na o hlahisa lihlahisoa tsa silicone tsa bongaka kapa thepa ea bareki, rabara ena ea silicone e kopana le maemo a holimo a pepeneneng.
GA-33 × 1 e fana ka matla a matla a mochini le ho hanyetsa ho lla, ho e etsa hore e be e loketseng ho sebelisoa lits'ebetsong tse boima. E sebelisoa haholo lihlahisoa tsa rabara tse tšoarellang joalo ka litiiso tsa bongaka, likarolo tsa likoloi, le thepa ea bareki e hlokang ho sebetsa ka ts'epo ha nako e ntse e ea. Sena se etsa hore e be khetho e ntle bakeng sa bahlahisi ba batlang rabara ea silicone e matla haholo.
Rabara ena ea silicone e bonaletsang haholo e fana ka ts'ebetso e ntle haholo, e nolofalletsang ho e etsa habonolo ho fihlela litlhoko tse ikhethang tsa moralo. Hore na o hloka likarolo tse rarahaneng tsa rabara ea silicone kapa tlhahiso e kholo, GA-33 × 1 e ts'ehetsa ho bopa ha rabara ka mokhoa o sebetsang hantle le tharollo ea rabara ea silicone. Sena se ntlafatsa linako tsa tlhahiso le ho thusa ho fokotsa litšenyehelo tsa tlhahiso, ho e etsa tharollo e nepahetseng bakeng sa likhoebo tsa B2B.
GA-33 × 1 rabara ea silicone e lumellana le litekanyetso tsa bohlokoa tsa tšireletso tsa machaba tse kang RoHS, REACH, le LFGB. Lisetifikeiti tsena li tiisa hore e bolokehile hore e ka sebelisoa liindastering tse kang tlhokomelo ea bophelo bo botle, ho ikopanya le lijo, le lisebelisoa tsa elektroniki, ho netefatsa boleng bo phahameng ka ho fetisisa tlhahisong ea lihlahisoa tsa rabara. Baetsi ba ka kholiseha hore lihlahisoa tsa bona li finyella litlhoko tsa ts'ireletso ea indasteri le tikoloho.
Rabara ena e pepeneneng ea silicone e sebelisoa haholo lits'ebetsong tsa bophelo bo botle, joalo ka li-pacifiers le li-nipples tsa botlolo ea bana, hammoho le thepa ea bareki. Ho lumellana ha eona le litekanyetso tsa polokeho le pepeneneng e phahameng ho etsa hore e be thepa e ratoang bakeng sa lihlahisoa tsa rabara tsa silicone tsa bongaka. E boetse e loketse ho theha likarolo tsa rabara tse bonaletsang, tse se nang chefo tse hlokang ts'ebetso e phahameng le polokeho.
GA-33 × 1 e fana ka khanyetso e ntle ea mocheso, e netefatsa ts'ebetso e tšepahalang libakeng tse nang le mocheso o feteletseng. Ho sa tsotellehe hore na e na le mocheso o phahameng kapa o tlaase, e boloka thepa ea eona, e etsa hore e tšoanelehe bakeng sa tšebeliso ea likoloi, lihlahisoa tsa silicone tsa boemo ba lijo, le likaroloana tsa rabara tsa bongaka tse hlokang ts'ebetso e tsitsitseng tlas'a maemo a thata.
Thepa ena ha e na chefo, hypoallergenic, 'me e bolokehile hore e ka sebelisoa lits'ebetsong tse bobebe. GA-33×1 e lumellana le litekanyetso tsa ts'ireletso ea lefats'e, e etsa hore e be e loketseng lihlahisoa tsa bana, lisebelisoa tsa bongaka, le lintho tse ling tse hlokolosi tsa bareki. E etselitsoe hore e bolokehe bakeng sa ho pepeseha nako e telele lits'ebetsong tsa bophelo bo botle le tsa maemo a lijo.
GA-33 × 1 silicone rabara e sebelisoa ho pholletsa le liindasteri tse fapaneng, ho kenyeletsoa likoloi, tsa bongaka, thepa ea bareki le lisebelisoa tsa elektroniki. Ho feto-fetoha ha eona le ts'ebetso e phahameng ho etsa hore e be khetho e phethahetseng bakeng sa likhoebo tse batlang litharollo tsa rabara tse pepeneneng tse sebetsang hantle tsa silicone tse fihlelang maemo a boima a indasteri.
Ka litharollo tsa eona tsa rabara tsa silicone tse tloaelehileng, pepeneneng e phahameng, le ho latela litekanyetso tsa machaba tsa polokeho, GA-33×1 ke khetho e tšepahalang bakeng sa likhoebo tse mafapheng a fapaneng. Hore na o etsa lihlahisoa tsa silicone tsa bongaka, likarolo tsa rabara ea likoloi, kapa thepa ea bareki, GA-33×1 e fana ka rabara e tšoarellang, e bonaletsang e netefatsang ts'ebetso le polokeho.
Q1: Ke litšebeliso life tse ka sehloohong tsa rabara ea silicone ea GA-33 × 1 e hlakileng haholo?
A1: GA-33×1 e loketse likarolo tsa rabara tse bonaletsang joalo ka li-pacifiers, litiiso tsa bongaka, le thepa e hlakileng ea bareki.
Q2: Na rabara ea silicone ea GA-33 × 1 e ka etsoa bakeng sa lits'ebetso tse ikhethileng?
A2: E, re fana ka litharollo tsa rabara tsa silicone tse ikamahanyang le moralo oa hau le litlhoko tsa ts'ebetso.
Q3: Na GA-33 × 1 e lumellana le litekanyetso tsa machaba tsa tšireletso?
A3: E, e kopana le litifikeiti tsa RoHS, REACH, le LFGB bakeng sa polokeho ea bophelo bo botle, lijo le lisebelisoa tsa elektroniki.
Q4: Ke liindasteri life tse atisang ho sebelisa rabara ea silicone ea GA-33 × 1?
A4: E sebelisoa haholo ho tsa bophelo bo botle, likoloi, thepa ea bareki, le lisebelisoa tsa elektroniki bakeng sa lits'ebetso tse sebetsang hantle.
Q5: Na GA-33 × 1 e fana ka nako e ntle ea nako e telele tlas'a mocheso o feteletseng?
A5: E, e hanyetsana le mocheso o phahameng le o tlaase, ho boloka ts'ebetso maemong a boima.
Q6: Na GA-33 × 1 ha e na chefo ebile e bolokehile bakeng sa lits'ebetso tse bobebe?
A6: E, rabara ena ea silicone ha e na chefo, hypoallergenic, 'me e bolokehile bakeng sa lihlahisoa tse bonolo tse kang li-pacifiers.
Q7: GA-33 × 1 e bapisoa joang le liraba tse ling tse pepeneneng tsa silicone?
A7: GA-33 × 1 e fana ka ponaletso e phahameng, matla, le ts'ebetso ea ts'ebetso bakeng sa lits'ebetso tse hlokang.
Q8: Na GA-33 × 1 e ka sebelisoa lits'ebetsong tsa ho ikopanya le lijo?
A8: E, e lumellana le LFGB mme e bolokehile bakeng sa lits'ebetso tsa maemo a lijo, e netefatsa boleng le polokeho.