Wowɔ ha: Fie » Nneɛma a wɔyɛ » Nneɛma a Wɔde Yɛ Nneɛma » VMQ Silicone a wɔde yɛ adwuma » GA-33×1 Silicone Rɔba a ɛyɛ mmerɛw yiye (Silica a ɛyɛ hu) (HCR)

loading a wɔde ahyɛ mu

Kyɛ ma:
facebook a wɔde kyɛ nsɛmma nhoma
twitter so a wɔde kyɛ ade
line kyɛfa button
wechat kyɛfa button
linkedin kyɛfa button
pinterest a wɔde kyekyɛ nneɛma
whatsapp kyɛfa button
kyɛ saa kyɛfa button yi

GA-33×1 Silicone Rɔba a Ɛma Nhumu Kɛse (Silica a ɛyɛ wusiw) (HCR) .

Dwumadi: nipple, sundries a ɛyɛ mmerɛw kɛse ne akwahosan ho nneɛma.
Nneɛma titiriw: transparence a ɛkorɔn, ahoɔden a ɛkorɔn, processability a ɛkyɛn so,twam nokwaredi a RoHS, REACH, ne LFGB.
 
Yɛyɛ GA-33 × 1 Highly Transparent Silicone Rubber (fumed Silica) (HCR) yɛfo na yɛde ma. Yɛde ano aduru a wɔayɛ ama nnwuma a ɛhwehwɛ sɛ wɔyɛ silicone rɔba a ɛyɛ mmerɛw na ɛyɛ adwuma yiye ma. Yɛn kuw no betumi ayɛ silicone rɔba a ɛwɔ nsɛm pɔtee a ɛfa ho de adi wo adwuma no ahiade ho dwuma. Yɛnam mfiridwuma a ɛkɔ anim ne mfiridwumayɛfo a wɔn ho akokwaw so hwɛ hu sɛ wɔde nneɛma a ɛkorɔn sen biara na wɔde bɛma ntɛmntɛm.
  • GA33×1 na ɛwɔ hɔ

Nea Ɛwɔ Hɔ:
Dodow:

Yɛn GA-33×1 Silicone Rɔba a Ɛma Nhumu Kɛse (Silica a ɛyɛ hu) (HCR) a Wɔde Di Dwuma


GA-33×1 yɛ silicone rɔba a ɛyɛ mmerɛw yiye a wɔde silica a ɛyɛ wusiw ayɛ, a wɔayɛ no titiriw ama nnwuma a ɛhwehwɛ sɛ ɛyɛ nea ɛda adi kɛse, ɛyɛ nea ɛyɛ mmerɛw, na ɛyɛ nea ɛyɛ den. Saa ade yi fata sɛ wɔde di dwuma wɔ nnwuma te sɛ kar, ɛlɛtrɔnik mfiri, nnuruyɛ mfiri, ne nneɛma afoforo a ɛyɛ adwuma yiye mu. Ɛde mfaso a ɛwɔ aniwa mu pefeeyɛ so ne mfiridwuma mu nneɛma soronko bom.


Wobɛtumi Sesa no sɛdeɛ Wo Nsɛm a Wɔakyerɛkyerɛ Mu no Ahyia

Sɛ́ silicone rɔba yɛfo a odi kan no, yɛde ano aduru a wɔayɛ ama w’adwuma ahiade ahorow ma. GA-33×1 silicone rɔba wɔ hɔ wɔ ahorow ahorow mu sɛnea ɛbɛyɛ a ɛne w’ahiade pɔtee hyia. Sɛ́ ebia wuhia elasticity a ɛkorɔn anaasɛ ahoɔden a ɛma wotetew mu no, yebetumi asiesie nnuru no ma ɛne wo nkyerɛkyerɛmu soronko no ahyia. Yɛasi yɛn bo sɛ yɛde B2B ano aduru a ɛwɔ adetɔfo som a ɛkyɛn so ne bere a wɔde bɛkɔ ntɛmntɛm bɛma.


Nhumu a Ɛkorɔn ma Nnwuma Ahorow Ahorow

GA-33×1 silicone rɔba no ma ahoɔden a ɛkɔ soro, na ɛma ɛyɛ pɛpɛɛpɛ ma nsɔano, gasket, nnuruyɛ mu nneɛma, ne afã horow a wɔanwene a ɛyɛ mmerɛw. Ɛdu nnwuma gyinapɛn a ɛyɛ katee so, hwɛ hu sɛ ɛyɛ papa ne adwumayɛ ma dwumadie a ɛho hia wɔ baabi a dwumadie ne afɛfɛdeɛ nyinaa ho hia.


Mfiri ne Ɔhyew Ho Nneɛma a Ɛkorɔn

Yɛn silicone rɔba no ma ahoɔden a ɛda nsow a ɛtwetwe, ɛtrɛw, na ɛko tia tetew, na ɛma ɛyɛ adwuma bere tenten wɔ mmeae a nhyɛso kɛse mpo. Esiane sɛ saa ade yi tumi gyina ɔhyew ano yiye nti, ɛyɛ nea ɛfata sɛ wɔde bedi dwuma wɔ mmeae a ɛhɔ yɛ hyew kɛse. Ɛyɛ nea eye titiriw ma kar afã horow, ɛlɛtrɔnik nneɛma, ne nnuruyɛ mfiri a ɛhwehwɛ sɛ ɛtra hɔ kyɛ na ɛyɛ nsakrae.


Sɔhwɛ: 1% a ɛyɛ aduru a wɔde sa yare (50% a wɔde DBPMH a wɔde ahyɛ silicone gum mu), 175° x 5min x 15MPa.


Nneɛma a wɔyɛ no parameters
Adwadeɛ GA-3331 na ɛwɔ hɔ
GA-3341 na ɛwɔ hɔ GA-3351 na ɛwɔ hɔ GA-3361 na ɛwɔ hɔ GA-3371 na ɛwɔ hɔ
Mmaeɛ Fann
Williamplasticity a wɔde yɛ nneɛma
155
200
220
260
280
Nneɛma a ɛyɛ den (Shor
30
40
50
60
70
Nsuo a ɛyɛ den(g/cm3) . 1.08
1.11
1.14
1.17
1.20
Ahoɔden a wɔde twe ade (MPa) .

9
10
10
10
9
Ntrɛwmu(%) . 850
750
650
550
400
Ahoɔden a ɛtetew mu (kN/m) . 20
22
25
30
25
Nneɛma a wɔde fa nsɛm mu(%) .
85
86
87
87
88


GA-33×1 Highly Transparent Silicone Rubber (fumed Silica) (HCR) yɛ ade a ɛyɛ adwuma pii a wɔayɛ ama nneɛma ahorow pii. Sɛnea ɛyɛ mmerɛw kɛse, ahoɔden a ɛkorɔn a ɛma nusu, ne ɔhyew a ɛko tia no ma ɛyɛ nea eye ma nnwuma a ɛhwehwɛ sɛ wotumi de ho to so, te sɛ kar, ɛlɛtrɔnik mfiri, ne nnuruyɛ mfiri. Yɛde ano aduru a wɔahyɛ da ayɛ ma de di nneɛma pɔtee a wɔhwehwɛ ho dwuma, hwɛ hu sɛ ɛyɛ adwuma yiye na ɛtra hɔ kyɛ wɔ dwumadie ahodoɔ mu. Sɛ́ silicone rɔba yɛfo a wogye wɔn di no, yɛde nneɛma a ɛkorɔn na ɛho ka sua a wɔayɛ ama w’ahiade ahorow ma.


Silicone Rɔba a Ɛyɛ Nwene Kɛse

GA-33 × 1 Silicone Rɔba a ɛyɛ mmerɛw kɛse (fumed Silica) (HCR) - Nneɛma atitiriw


Nhumu a Ɛkorɔn a Wɔde Di Dwuma a Ɛda Hɔ

Wɔayɛ GA-33 × 1 silicone rɔba ama nea ɛda adi kɛse, na ɛma ɛyɛ pɛpɛɛpɛ ma silicone rɔba a emu da hɔ nneɛma. Saa ade yi ye ma nneɛma te sɛ pacifiers, transparent seals, ne rɔba nneɛma afoforo a emu da hɔ wɔ baabi a ɛho hia sɛ emu da hɔ na ahoɔden wom. Sɛ́ ebia woreyɛ nnuruyɛ mu silicone nneɛma anaa nneɛma a wɔde di dwuma no, saa silicone rɔba yi du gyinapɛn a ɛkorɔn sen biara a ɛma wohu nneɛma a ɛda adi pefee no ho.


Mfiridwuma mu Ahoɔden a Ɛkyɛn So

GA-33×1 ma mfiri ahoɔden a ɛkyɛn so ne nea ɛko tia tetew, na ɛma ɛyɛ nea eye sɛ wɔde bedi dwuma wɔ nneɛma a ɛyɛ den mu. Wɔde di dwuma kɛse wɔ rɔba nneɛma a ɛyɛ den te sɛ nnuruyɛ mu nsɔano, kar nneɛma, ne nneɛma a wɔde di dwuma a ɛsɛ sɛ ɛyɛ adwuma yiye bere a bere kɔ so no. Eyi ma ɛyɛ nea eye sen biara ma wɔn a wɔyɛ nneɛma a wɔhwehwɛ silicone rɔba a ahoɔden wom kɛse no.


Nnwuma Kɛse a Wɔde Di Dwuma

Saa silicone rɔba a ɛda adi kɛse yi ma wotumi di ho dwuma yiye, na ɛma ɛyɛ mmerɛw sɛ wɔbɛsakra nneɛma ma wɔadi adwini ahiade pɔtee bi ho dwuma. Sɛ́ ebia wuhia silicone rɔba afã horow a ɛyɛ den anaasɛ wɔyɛ no kɛse no, GA-33×1 boa rɔba a wɔyɛ no yiye ne silicone rɔba ano aduru a wɔayɛ no sɛnea wɔpɛ. Eyi ma bere nhyehyɛe a wɔde yɛ nneɛma tu mpɔn na ɛboa ma wɔtew nneɛma a wɔyɛ ho ka so, na ɛma ɛyɛ ano aduru a eye ma B2B nnwuma.


Amanaman Ntam Gyinapɛn ahorow a Wodi So

GA-33×1 silicone rɔba di amanaman ntam ahobammɔ gyinapɛn a ɛho hia te sɛ RoHS, REACH, ne LFGB so. Saa adansedi ahorow yi ma awerɛhyem sɛ ahobammɔ wom sɛ wɔde bedi dwuma wɔ nnwuma te sɛ akwahosan ho nhyehyɛe, aduan a wɔde di nkitaho, ne ɛlɛtrɔnik mfiri mu, na ɛma wɔhwɛ hu sɛ ɛyɛ nea ɛkorɔn sen biara wɔ rɔba nneɛma a wɔyɛ mu. Wɔn a wɔyɛ nneɛma no betumi anya ahotoso sɛ wɔn nneɛma no di nnwuma no ahobammɔ ne nneɛma a atwa yɛn ho ahyia ho ahwehwɛde ahorow ho dwuma.


Ɛyɛ papa ma Akwahosan ne Nneɛma a Wɔde Di Dwuma

Wɔde saa silicone rɔba a ɛyɛ mmerɛw yi di dwuma kɛse wɔ akwahosan ho nneɛma te sɛ nea wɔde ma nufu ne nkokoaa toa mu nufu, ne nneɛma a wɔde di dwuma mu. Sɛnea ɛne ahobammɔ gyinapɛn ahorow hyia ne sɛnea ɛda adi kɛse no ma ɛyɛ ade a wɔpɛ sɛ wɔde yɛ nnuru a wɔde yɛ silicone rɔba. Ɛsan nso yɛ papa ma rɔba afã horow a ɛda adi pefee, a awuduru nnim a ɛhwehwɛ sɛ wɔyɛ adwuma yiye na ahobammɔ wom.


Ɔhyew a Ɛko Tia Nneɛma a Atwa Yɛn Ho Ahyia a Ɛyɛ Den

GA-33×1 ma ɔhyew a ɛko tia a ɛkyɛn so, na ɛma wotumi de ho to so sɛ ɛyɛ adwuma wɔ mmeae a ɔhyew a ɛboro so wɔ hɔ. Sɛ́ ebia ɛwɔ ɔhyew a ɛkɔ soro anaasɛ ɛba fam mu no, ɛkɔ so kura ne su ahorow mu, na ɛma ɛfata sɛ wɔde di dwuma wɔ kar mu, silicone nneɛma a ɛyɛ aduan, ne nnuruyɛ mu rɔba nneɛma a ɛhwehwɛ sɛ wɔyɛ adwuma bere nyinaa wɔ tebea horow a emu yɛ den mu.


Ɛnyɛ awuduru na Ahobammɔ Ma Nnwuma a Ɛyɛ Nkate a Wɔde Di Dwuma

Saa ade yi nyɛ awuduru, ɛnyɛ nea ɛma obi ho yɛ no yaw, na asiane biara nni ho sɛ wɔde bedi dwuma wɔ nneɛma a ɛyɛ mmerɛw mu. GA-33×1 di wiase nyinaa ahobammɔ gyinapɛn ahorow so, na ɛma ɛyɛ nea eye ma mmofra nneɛma, nnuruyɛ mfiri, ne nneɛma afoforo a ɛho hia a wɔde di dwuma. Wɔayɛ no sɛnea ɛbɛyɛ a asiane biara nni ho sɛ wɔde bɛto hɔ bere tenten wɔ akwahosan ne aduan a wɔde di dwuma mu.


Nneɛma a Wɔde Di Dwuma a Wɔde Di Dwuma a Ɛwɔ Adwuma pii

Wɔde GA-33×1 silicone rɔba di dwuma wɔ nnwuma ahorow pii mu, a kar, aduruyɛ, nneɛma a wɔde di dwuma, ne ɛlɛtrɔnik mfiri ka ho. Ne tumi a ɛyɛ adwuma pii ne sɛnea ɛyɛ adwuma yiye no ma ɛyɛ nea ɛfata ma nnwuma a wɔrehwehwɛ silicone rɔba ano aduru a ɛyɛ adwuma yiye a ɛda adi pefee a ɛne mfiridwuma gyinapɛn ahorow a ɛyɛ den hyia.


Ɛnam ne silicone rɔba ano aduru a wɔayɛ no sɛnea wɔpɛ, nea ɛda adi kɛse, na ɛne amanaman ntam ahobammɔ gyinapɛn ahorow hyia nti, GA-33×1 yɛ nea wotumi de ho to so ma nnwuma a ɛwɔ nnwuma ahorow mu. Sɛ́ ebia woreyɛ nnuruyɛ mu silicone nneɛma, kar rɔba afã horow, anaa nneɛma a wɔde di dwuma no, GA-33×1 de silicone rɔba a ɛyɛ den na ɛda adi pefee a ɛma ɛyɛ adwuma bere nyinaa na ahobammɔ wom ma.


Nsɛmmisa ne Mmuae a Wɔtaa Bisa


Q1: Dɛn ne nneɛma atitiriw a wɔde GA-33×1 silicone rɔba a ɛyɛ mmerɛw kɛse di dwuma?
A1: GA-33 × 1 yɛ papa ma transparent rɔba afã horow te sɛ pacifiers, aduruyɛ nsɔano, ne pefee consumer nneɛma.


Q2: So wobetumi ayɛ GA-33 × 1 silicone rɔba ama dwumadie pɔtee bi?
A2: Yiw, yɛde amanneɛbɔ silicone rɔba ano aduru a wɔayɛ ama wo nhyehyɛe ne adwumayɛ ahiade ahorow ma.


Q3: So GA-33×1 ne amanaman ntam ahobammɔ gyinapɛn ahorow hyia?
A3: Yiw, ɛne RoHS, REACH, ne LFGB adansedi ahorow a ɛfa ahobammɔ ho wɔ akwahosan, aduan, ne ɛlɛtrɔnik mfiri mu no hyia.


Q4: Nnwuma bɛn na wɔtaa de GA-33×1 silicone rɔba di dwuma?
A4: Wɔde di dwuma kɛse wɔ akwahosan, kar, nneɛma a wɔde di dwuma, ne ɛlɛtrɔnik mfiri a wɔde yɛ adwuma a ɛyɛ adwuma yiye mu.


Q5: So GA-33×1 ma ɛtra hɔ kyɛ yiye wɔ ɔhyew a ano yɛ den ase?
A5: Yiw, ɛko tia ɔhyew a ɛkɔ soro ne nea ɛba fam, na ɛma ɛyɛ adwuma wɔ tebea horow a emu yɛ den mu.


Q6: So GA-33×1 nyɛ awuduru na ahobammɔ wom ma dwumadie a ɛyɛ mmerɛw?
A6: Yiw, saa silicone rɔba yi nyɛ awuduru, ɛnyɛ nea ɛma obi ho yɛ no yaw, na ahobammɔ wom ma nneɛma a ɛyɛ mmerɛw te sɛ pacifiers.


Q7: Sɛ wɔde GA-33×1 toto silicone rɔba afoforo a ɛyɛ mmerɛw ho a, ɛyɛ dɛn?
A7: GA-33 × 1 ma superior transparency, ahoɔden, ne dwumadie adwumayɛ ma ahwehwɛdeɛ applications.


Q8: So wobetumi de GA-33×1 adi dwuma wɔ aduan a wɔde di nkitaho mu?
A8: Yiw, ɛne LFGB hyia na ahobammɔ wom ma aduan a wɔde di dwuma, na ɛhwɛ hu sɛ ɛyɛ papa na ahobammɔ wom.

Dada: 
Deɛ ɛdi hɔ: 

NKYERƐKYERƐMU A ƐYƐ NTƐM

NKYERƐKYERƐMU A ƐFA NKYERƐKYERƐMU HO

Fa ka ho: No.33, Ɔkwan 159, Taiye Kwan, Fengxian Mantam, Shanghai
Tɛlɛ / WhatsApp / Skype: +86 15221953351 wobɛtumi akyerɛw wo din
Nneɛma a wɔde yɛ adwuma     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap a Wɔde Di Dwuma |   Kokoam Nsɛm Ho Nhyehyɛe | Mmoa a Wɔde Ma Leadong na ɛwɔ hɔ.