GA33×1
| Kuwanikwa: | |
|---|---|
| Huwandu: | |
GA-33 × 1 inoonekera zvakanyanya silicone rabha yakagadzirwa nefumed silica, yakanyatsogadzirirwa maapplication anoda kujeka kwepamusoro, kuchinjika, uye kusimba. Ichi chigadzirwa chakakodzera kushandiswa mumaindasitiri akadai semotokari, zvemagetsi, zvigadziriso zvekurapa, uye zvimwe zvekushandisa zvakanyanya. Iyo inosanganisa mabhenefiti ekujekesa kwemaziso neakasarudzika ma mechanical properties.
Semugadziri anotungamira silicone rabha, isu tinopa yakagadziridzwa mhinduro kune rako bhizinesi zvido. GA-33 × 1 silicone rabha inowanikwa mumagiredhi akasiyana kuti ienderane nezvaunoda chaizvo. Kunyangwe iwe uchida yakakwira elasticity kana yakawedzera simba rekubvarura, isu tinokwanisa kugadzirisa iyo dhizaini kuti isangane neyako yakasarudzika zvirevo. Isu takazvipira kupa B2B mhinduro neakanakisa sevhisi yevatengi uye nekukurumidza kuburitsa nguva.
Iyo GA-33 × 1 silicone rabha inopa yakakwira transmittance, ichiita kuti ive yakakwana kune zvisimbiso, gaskets, zvekurapa zvinoumba, uye akajeka akaumbwa zvikamu. Iyo inosangana neyakaomesesa indasitiri zviyero, kuve nechokwadi chemhando uye mashandiro ezvikumbiro zvakakosha uko zvese basa uye aesthetics zvakakosha.
Yedu silicone rabha inopa yakasarudzika simba rekusimba, kurebesa, uye kubvarura kuramba, kuve nechokwadi chekuita kwenguva refu kunyangwe munzvimbo dzakanyanya-kushushikana. Nepamusoro-soro yekudzivirira kupisa, chinhu ichi chakanakira kushandiswa munzvimbo dzepamusoro-soro. Yakanyanya kunaka kune mota, zvikamu zvemagetsi, uye zvishandiso zvekurapa zvinoda kusimba uye kuchinjika.
Muedzo: 1% yekurapa mumiririri (50% paste yeDBPMH musilicone gum), 175 ° x 5min x 15MPa.
| Product parameters | |||||
| Product | GA-3331 |
GA-3341 | GA-3351 | GA-3361 | GA-3371 |
| Chitarisiko | Transparent | ||||
| Williamplasticity |
155 |
200 |
220 |
260 |
280 |
| Kuoma (ShoreA) |
30 |
40 |
50 |
60 |
70 |
| Density(g/cm3) | 1.08 |
1.11 |
1.14 |
1.17 |
1.20 |
| Tensile simba (MPa) |
9 |
10 |
10 |
10 |
9 |
| Elongation(%) | 850 |
750 |
650 |
550 |
400 |
| Simba rekubvarura (kN/m) | 20 |
22 |
25 |
30 |
25 |
| Transmittance(%) |
85 |
86 |
87 |
87 |
88 |
GA-33 × 1 Yakanyanya Kujeka Silicone Rubber (fumed Silica) (HCR) chinhu chinogoneka chakagadzirirwa kuwanda kwekushandisa. Kujeka kwayo kwepamusoro, simba rekubvarura repamusoro, uye kudzivirira kupisa kunoita kuti ive yakanakira maindasitiri anoda kuvimbika, senge mota, zvemagetsi, uye zvigadzirwa zvekurapa. Isu tinopa zvigadziriso zvetsika kuti zvisangane nezvinodiwa zvechigadzirwa, kuve nechokwadi chekuita kwakanaka uye kusimba mumashandisirwo akasiyana siyana. Semugadziri akavimbika wesilicone rabha, tinoendesa zvigadzirwa zvepamusoro-soro, zvinodhura zvakagadzirirwa zvinoenderana nezvaunoda.

GA-33 × 1 silicone rabha yakagadzirirwa kujeka kwakanyanya, ichiita kuti ive yakakwana kune yakajeka silicone rubber zvigadzirwa. Ichi chinyorwa chakanakira zvinhu zvakadai sepacifiers, zvisimbiso zvakajeka, uye zvimwe zvikamu zverabha zvakajeka apo kujekesa uye simba zvakakosha. Kunyangwe iwe uri kugadzira zvigadzirwa zvesilicone yezvokurapa kana zvinhu zvevatengi, iyi silicone rabha inosangana nemhando yepamusoro yekubuda pachena.
GA-33 × 1 inopa yakanakisa mechaniki simba uye kubvarura kuramba, zvichiita kuti ive yakanakira kushandiswa mukuda maapplication. Inoshandiswa zvakanyanya muzvigadzirwa zverabha zvinogara sezvisimbiso zvekurapa, zvinhu zvemotokari, uye zvinhu zvevatengi zvinoda kuita zvakavimbika nekufamba kwenguva. Izvi zvinoita kuti ive sarudzo yakanakisa yevagadziri vanotsvaga yakakwirira-simba silicone rabha.
Iyi yakanyanya kujeka silicone rabha inopa yakanakisa processability, ichigonesa nyore kugadzirisa kuti isangane neyakagadzirirwa dhizaini zvinodiwa. Kunyangwe iwe uchida yakaoma silicone yerubha zvikamu kana yakakura-yakakura kugadzirwa, GA-33 × 1 inotsigira inoshanda rabha kuumbwa uye tsika silicone rabha mhinduro. Izvi zvinovandudza nguva dzekugadzira uye zvinobatsira kuderedza mutengo wekugadzira, zvichiita kuti ive mhinduro yakanaka kumabhizinesi eB2B.
GA-33 × 1 silicone rabha inoenderana neakakomba epasi rose kuchengetedza zviyero seRoHS, REACH, uye LFGB. Izvi zvitupa zvinovimbisa kuti zvakachengeteka kushandiswa mumaindasitiri akadai sehutano, kubata chikafu, uye zvemagetsi, kuve nechokwadi chemhando yepamusoro mukugadzira zvigadzirwa zverabha. Vagadziri vanogona kuva nechivimbo chekuti zvigadzirwa zvavo zvinosangana nekuchengetedza indasitiri uye zvinodiwa zvezvakatipoteredza.
Iyi yakajeka silicone rabha inoshandiswa zvakanyanya mukuchengetedza hutano mashandisirwo, senge pacifiers uye bhodhoro remwana mazamu, pamwe chete muzvinhu zvevatengi. Kutevedzera kwayo mitemo yekuchengetedza uye kujeka kwepamusoro kunoita kuti ive chinhu chinofarirwa kune zvekurapa silicone rabha zvigadzirwa. Yakanakirawo kugadzira inoonekera, isina-chepfu yerubha zvinhu zvinoda kushanda kwepamusoro uye kuchengetedzeka.
GA-33 × 1 inopa yakanakisa tembiricha kuramba, kuve nechokwadi chekuita kwakavimbika munzvimbo dzine tembiricha yakanyanyisa. Ingave yakafumurwa kune tembiricha yakakwira kana yakaderera, inochengetedza zvimiro zvayo, ichiita kuti ive yakakodzera kushandiswa mumotokari kunyorera, chikafu-giredhi silicone zvigadzirwa, uye zvekurapa zverabha zvikamu zvinoda kushanda kwakafanana pasi pemamiriro akaomarara.
Ichi chinyorwa hachina chepfu, hypoallergenic, uye yakachengeteka kuti ishandiswe mumashandisirwo akajeka. GA-33 × 1 inopindirana nemitemo yekuchengetedza pasi rose, ichiita kuti ive yakanakira zvigadzirwa zvevana, zvishandiso zvekurapa, uye zvimwe zvinonzwisa tsitsi zvevatengi. Yakagadzirirwa kuve yakachengeteka kuratidzwa kwenguva refu muhutano hwehutano uye chikafu-giredhi maapplication.
GA-33 × 1 silicone rabha inoshandiswa kune akasiyana maindasitiri, anosanganisira emotokari, ekurapa, zvinhu zvevatengi, uye zvemagetsi. Kuita kwayo kwakasiyana-siyana uye kuita kwepamusoro kunoita kuti ive sarudzo yakanaka kune mabhizinesi ari kutsvaga yepamusoro-inoshanda yakajeka silicone rabha mhinduro dzinosangana nezvinodiwa zvemaindasitiri.
Iine yakajairwa silicone rabha mhinduro, kujeka kwepamusoro, uye kutevedzera mitemo yekuchengetedza pasi rose, GA-33 × 1 isarudzo yakavimbika kumabhizinesi ari muzvikamu zvakasiyana. Kunyangwe iwe uri kugadzira zvigadzirwa zvesilicone yezvokurapa, zvinhu zverabha zvemotokari, kana zvinhu zvevatengi, GA-33 × 1 inopa yakasimba, yakajeka silicone rabha inova nechokwadi chekushanda uye kuchengetedzeka.
Q1: Ndeapi mashandisirwo makuru eGA-33 × 1 akanyanya kujeka silicone rubha?
A1: GA-33 × 1 yakanakira zvinhu zverabha zvakajeka senge pacifiers, zvisimbiso zvekurapa, uye zvinhu zvakajeka zvevatengi.
Q2: Ko GA-33 × 1 silicone rabha inogona kugadzirwa kune chaiwo maapplication?
A2: Hongu, isu tinopa tsika silicone rabha mhinduro dzakagadzirirwa dhizaini yako uye kuita zvinodiwa.
Q3: GA-33 × 1 inowirirana nemitemo yekuchengetedzwa kwenyika?
A3: Hongu, inosangana neRoHS, REACH, uye LFGB zvitupa zvekuchengetedza hutano, chikafu, uye zvemagetsi.
Q4: Ndeapi maindasitiri anowanzo kushandisa GA-33 × 1 silicone rabha?
A4: Inoshandiswa zvakanyanya mukuchengetedza hutano, mota, zvinhu zvevatengi, uye zvemagetsi zvekushandisa zvakanyanya.
Q5: Ko GA-33 × 1 inopa kusimba kwakanaka pasi pekupisa kwakanyanya?
A5: Hongu, inopikisa kutonhora kwepamusoro uye kwakadzika, kuchengetedza kushanda mumamiriro ezvinhu anoda.
Q6: Iyo GA-33 × 1 isiri-chepfu uye yakachengeteka kune yakaoma application?
A6: Hongu, iyi silicone rabha haina chepfu, hypoallergenic, uye yakachengeteka kune zvigadzirwa zvinonzwisisika sepacifiers.
Q7: GA-33 × 1 inofananidzwa sei nemamwe akajeka silicone rubbers?
A7: GA-33 × 1 inopa kujeka kwepamusoro, simba, uye kugadzirisa mashandiro ezvikumbiro zvinoda.
Q8: Ko GA-33 × 1 inogona kushandiswa mumashandisirwo ekudya?
A8: Hongu, inoenderana neLFGB uye yakachengeteka kune chikafu-giredhi maapplication, kuve nechokwadi chemhando uye chengetedzo.