GA-32 × 0 General Purpose Silicone Rubber, e entsoeng ke Shanghai Herchy Rubber Co., Ltd, e etselitsoe ho finyella litlhoko tse ngata tsa indasteri. Ka limaraka tse fapaneng, ho kenyeletsoa GA-3230 ho isa GA-3280, e fana ka ts'ebetso e fapaneng lits'ebetsong tse fapaneng. Rabara ena ea silicone e sebetsang hantle haholo e loketse ho tiisa, ho kenya gasketing le ho kenya letsoho liindastering tse fapaneng tse kang tsa likoloi, tsa elektroniki le tsa kaho.
Rabara ena ea silica silicone e nang le mosi e bonts'a ho tenyetseha le ho tšoarella ha nako e telele, e e etsa hore e tšoanele maemo a mocheso o phahameng le o tlase. E fana ka matla a ikhethang a ho tiea, ho lelefatsa, le ho hanyetsa meokho, ho netefatsa ts'ebetso ea nako e telele le tlas'a maemo a boima. E sebelisoa hangata lits'ebetsong tse hlokang ho tenyetseha le matla, joalo ka litiiso tsa silicone, li-gasket tsa silicone, le likarolo tsa elastomeric.
Rabara ea silicone e feto-fetohang e fumaneha maemong a thata a fapaneng, ho tloha ho 30 Shore A ho isa 80 Shore A, e u fang bokhoni ba ho khetha mophato o nepahetseng ka ho fetisisa bakeng sa litlhoko tsa hau tse ikhethang. Ka bongata bo fapaneng le matla a ho tsitsa, letoto la GA-32 × 0 le ka etsoa bakeng sa mefuta e fapaneng ea lits'ebetso tsa indasteri le tsa khoebo.
Letoto la GA-32 × 0 le na le mekhoa e mengata e fapaneng, e leng se etsang hore e be khetho e nepahetseng bakeng sa tharollo ea rabara ea silicone e tloaelehileng. Hore na o hloka rabara ea silicone e tenyetsehang bakeng sa likarolo tsa koloi, lisebelisoa tsa motlakase, kapa lisebelisoa tsa kaho, sehlahisoa sena se fana ka ts'ebetso e ikhethang mefuteng e mengata e fapaneng ea ts'ebeliso.
Teko: 1% ea moemeli oa phekolo (50% peista ea DBPMH ka silicone gum), 175 ° x 5min x 15MPa.
| Lihlahisoa tsa lihlahisoa | ||||||
| Sehlahisoa | GA-3230 |
GA-3240 | GA-3250 | GA-3260 | GA-3270 | GA-3280 |
| Ponahalo | Translucent | |||||
| Williamplasticity |
140 |
180 |
210 |
240 |
280 |
310 |
| Ho thatafala (LebopoA) |
30 |
40 |
50 |
60 |
70 |
80 |
| Boima ba 'mele(g/cm3) | 1.08 |
1.11 |
1.14 |
1.17 |
1.20 |
1.22 |
| Tensilestrength (MPa) |
9 |
9.5 |
11 |
10.5 |
10.5 |
9 |
| Elongation(%) | 900 |
700 |
650 |
600 |
450 |
350 |
| Matla a metsi (kN/m) | 18 |
22 |
25 |
30 |
30 |
30 |
Ka letoto la GA-32 × 0 General Purpose Silicone Rubber, u fumana litharollo tse ka tšeptjoang, tse ka khonehang bakeng sa lits'ebetso tse fapaneng tsa indasteri. Hore na o batla rabara ea silicone bakeng sa ho etsoa, rabara ea silicone e matla haholo, kapa lisebelisoa tsa rabara tse tenyetsehang bakeng sa ho tiisoa, lihlahisoa tsa rona li fana ka ts'ebetso e ntle ka ho fetisisa 'marakeng.
Ikopanye le rona kajeno ho buisana ka litlhoko tsa projeke ea hau, 'me re tla hlophisa rabara e phethahetseng ea silicone ea HCR ho lumellana le litlhoko tsa hau.

GA-32 × 0 General Purpose Silicone Rubber, e nang le silika e tukang, ke thepa e sebetsang ka mefuta e mengata e loketseng mefuta e mengata ea lits'ebetso tsa indasteri. E fana ka ts'ebetso e phahameng 'me e tšeptjoa ke liindasteri tse hlokang li-elastomer tse tšoarellang le tse tenyetsehang. Ka tlase ke lintlha tsa bohlokoa tse etsang hore GA-32 × 0 e be khetho e tšepahalang.
GA-32 × 0 e sebelisoa ho hlahisa lihlahisoa tse fapaneng tsa rabara tsa silicone tse kang liqibi, li-gaskets le liphahlo tse sireletsang. E sebetsa ka ho khetheha liindastering tse kang ho etsa likoloi, lisebelisoa tsa elektroniki le thepa ea bareki, e leng se etsang hore e be khetho e tsebahalang bakeng sa lits'ebetso tse akaretsang.
Rabara ena ea silicone e bonts'a linako tsa ho folisa ka potlako, e ntlafatsa ts'ebetso ea tlhahiso le ho fokotsa nako. Hore na o etsa likarolo tsa silicone bakeng sa litiiso tsa likoloi kapa li-insulation tsa motlakase, GA-32 × 0 e fana ka pheko e potlakileng ho kopana le kemiso ea tlhahiso e batloang haholo.
GA-32 × 0 e fana ka matla a ikhethang, e netefatsa ts'ebetso e tšoarellang halelele lits'ebetsong tse boima. Thepa ena e etsa hore e be e loketseng bakeng sa likarolo tse tlas'a khatello ea mochini, joalo ka liqibi, li-gaskets le likoahelo tse sireletsang.
Ho sebetsa habonolo ho etsa hore GA-32 × 0 e loketse meralo e fapaneng ea hlobo. Litšobotsi tsa eona tse hlahelletseng tsa phallo li netefatsa liphetho tse tsitsitseng le lihlahisoa tsa boleng bo holimo, tse phethahetseng bakeng sa mekhoa e tloaelehileng le ea tlhahiso ea bongata.
GA-32 × 0 rabara ea silicone e kopana le litekanyetso tsa bohlokoa tsa taolo ea machaba tse kang litifikeiti tsa RoHS, REACH, le LFGB. Lisetifikeiti tsena li netefatsa hore thepa e bolokehile hore e ka sebelisoa lits'ebetsong tsa maemo a lijo, lisebelisoa tsa bongaka le lihlahisoa tse hlokang ho lateloa ka thata.
GA-32 × 0 e bonts'a matla a makatsang a ho lla, ho netefatsa ho tšoarella le tlas'a maemo a thata. E loketse ka ho khetheha bakeng sa litiiso tsa indasteri le lihlahisoa tse ling tse hlokang ho mamella ho senyeha ha nako le nako.
GA-32 × 0 e hanyetsana haholo le mocheso o feteletseng, ho boloka botšepehi ba eona ho pholletsa le mefuta e mengata ea mocheso. Sena se etsa hore e be se loketseng bakeng sa ho sebelisoa lits'ebetsong tse kang likarolo tsa likoloi, sebaka sa sefofane, le lisebelisoa tsa elektroniki, moo botsitso bo phahameng le bo tlase ba mocheso bo leng bohlokoa.
Ka mefuta e fapaneng ea limaraka tse thata, GA-32 × 0 e ka hlophisoa ho latela litlhoko tsa hau tse ikhethileng. Hore na o batla elastomer e bonolo bakeng sa litiiso kapa boemo bo tiileng bakeng sa li-gaskets, rabara ena ea silicone e ka hlophisoa hore e lumellane le lintlha tsa hau hantle.
Shanghai Herchy Rubber Co., Ltd. ke moetsi ea ka sehloohong le morekisi oa rabara ea silicone le lihlahisoa tse ling tsa elastomer. Re tsepamisitse maikutlo ho thepa ea boleng bo holimo, re sebeletsa liindasteri tse kang tsa makoloi, sefofane, bongaka le thepa ea bareki. Sehlopha sa rona se nang le phihlelo se tiisa hore sehlahisoa se seng le se seng se finyella litekanyetso tse phahameng ka ho fetisisa tsa boleng le ts'ebetso, ho thusa bareki ba rona ho finyella lipakane tsa bona ka tharollo e tšepahalang. Hore na o batla li-silicone metsoako, litlolo tse ikhethileng, kapa mofuta o itseng oa rabara, re fana ka litharollo tse feto-fetohang le tse etselitsoeng litlhoko tsa khoebo ea hau.
Shanghai Herchy Rubber Co., Ltd., re ikemiselitse ho fana ka bokhabane le boqapi, ho netefatsa hore lihlahisoa tsohle tsa rona, ho kenyeletsoa GA-32×0, li fihlela litlhoko tsa hau hantle le ho thusa khoebo ea hau pele.