Aw bɛ yan: So » Fɛn minnu bɛ dilan » Sintezi Lastikuw » VMQ Silikɔni ye » GA-33×1 Silicone Rubber transparent kosɛbɛ (Silica fumé) (HCR)

doni tali

Share to:
facebook tilali butɔni
twitter tilali butɔni
layini tila-tila butɔni
wechat tila-tila butɔni
linkedin tila-tila butɔni
pinterest tila-tila butɔni
whatsapp tilali butɔni
sharethis nin tila-tila butɔni

GA-33×1 Silicone Rubber min bɛ kɛnɛya kosɛbɛ (Silica fumé) (HCR) .

A kɛcogo: sinji, sundries minnu bɛ kɛnɛya kosɛbɛ ani kɛnɛya furaw.
Fɛn kolomaw: kɛnɛya ka bon, fanga ka bon, baarakɛcogo ɲuman,tɛmɛ RoHS, REACH, ani LFGB tiɲɛni kan.
 
An ye GA-33×1 Silicone Rubber (Silica fumed) (HCR) dilanbaga ye ani a feerela dannamɔgɔ ye. An bɛ furaw di minnu bɛ bɛn iziniw ma minnu bɛ silikoni lastikuw fɛnw wajibiya minnu bɛ kɛnɛya, minnu bɛ baara kɛ kosɛbɛ. An ka jɛkulu bɛ se ka silikɔni lastikuw dilan ni a ɲɛfɔcogo tigitigiw ye walasa k’aw ka poroze magow ɲɛ. Ni fɛɛrɛ kuraw ni ɛntɛrinɛti injiniyɛri dɔnbagaw ye, an b’a to fɛnw bɛ se ka kɛ cogo ɲuman na ani ka fɛnw di teliya la.
  • GA33×1 ye

A sɔrɔli:
Hakɛ: .

An ka GA-33×1 Silicone Rubber (Silicone fumé) (HCR) min bɛ kɛnɛya kosɛbɛ, o jirali .


GA-33×1 ye silikoni lastikuw ye min bɛ kɛnɛya kosɛbɛ, min dilannen don ni silisi sisilen ye, min dabɔra kɛrɛnkɛrɛnnenya la baara kama minnu bɛ kɛnɛyako caman wajibiya, ka fɛn caman sɛgɛsɛgɛ, ani ka se ka muɲu. Nin fura in bɛnnen don ka baara kɛ ni iziniw ye i n’a fɔ mobili, ɛntɛrinɛti, furakɛli minɛnw, ani baara wɛrɛw minnu bɛ baara kɛ kosɛbɛ. A bɛ ɲɛnayeli jɛlen nafaw fara ɲɔgɔn kan ni masinko danfaralenw ye.


A bɛ se ka ladilan ka kɛɲɛ ni I ka fɛn ɲɛfɔlenw ye

Anw minnu ye silikɔni lastikuw dilanko ɲɛmɔgɔba ye, an bɛ furaw di aw ma minnu bɛ kɛ ka kɛɲɛ ni aw ka jago magow ye. GA-33×1 silikɔni lastikuw bɛ sɔrɔ suguya wɛrɛw la walasa ka bɛn aw ka ɲininiw tigitigi ma. Aw mago bɛ elasticité caman na wo, walima ɲɛji fanga bonyalen wo, an bɛ se ka a furakɛcogo labɛn ka kɛɲɛ ni aw ka fɛn kɛrɛnkɛrɛnnenw ye. An b’an jija ka B2B furaw di ni kiliyanw dɛmɛni ɲuman ye ani ni fɛnw lase waati teliya ye.


Transparence haute pour les applications différentes

GA-33×1 silikɔni lastikuw bɛ fɛnw cicogo caman di, o b’a to a dafalen don sigilanw, gaziw, furakɛli yɔrɔw, ani yɔrɔ nɔgɔlenw na minnu dilannen don. A bɛ izini sariya gɛlɛnw dafa, ka jogoɲumanya ni baarakɛcogo sabati baarakɛcogo kɔrɔw kama yɔrɔ minnu na baarakɛcogo ni cɛɲi fila bɛɛ nafa ka bon.


Masina ni funteni nafaw ka bon kosɛbɛ

An ka silikɔni lastikuw bɛ fanga ɲumanba di, ka janya, ani ka ɲɛji bɔ, o bɛ a to a ka baara kɛ waati jan kɔnɔ hali ni degunba bɛ yɔrɔ minnu na. Ni funteni kunbɛncogo ka fisa, nin fɛn in dafalen don walasa ka baara kɛ ni a ye yɔrɔw la minnu funteni ka bon. A ka ɲi kɛrɛnkɛrɛnnenya la mobili yɔrɔw, ɛntɛrinɛti yɔrɔw ani furakɛli minɛnw kama minnu bɛ muɲu ani ka fɛn caman sɛgɛsɛgɛ.


Kɔrɔbɔli : 1% furakɛlifɛn (DBPMH 50% paste silikɔni gomu kɔnɔ), 175° x 5min x 15MPa.


Fɛn dilannenw ka paramɛtiriw
Ka kɛ GA-3331 ye
GA-3341 ye GA-3351 ye GA-3361 ye GA-3371 ye
Yecogo Jɛlen
Williamplasticity (Wiliamplasticité) ye
155
200
220
260
280
Gɛlɛya (KɔgɔjidaA) .
30
40
50
60
70
Densité(g/cm3) ye. 1.08
1.11
1.14
1.17
1.20
Sɛgɛsɛgɛli fanga (MPa) .

9
10
10
10
9
Janya(%) . 850
750
650
550
400
Ɲɛjibɔ fanga (kN/m) . 20
22
25
30
25
Tɛmɛsira(%) .
85
86
87
87
88


GA-33×1 Silicone Rubber (Silica fumed) (HCR) ye fɛn ye min bɛ se ka kɛ fɛn caman ye, min dilannen don baara caman kama. A ka kɛnɛya ka bon, a ɲɛjibɔ fanga ka bon, ani a ka funteni kɛlɛli b’a to a ka ɲi kosɛbɛ iziniw ma minnu bɛ dannaya ɲini, i n’a fɔ mobili, ɛntɛrinɛti ani furakɛli minɛnw. An bɛ fɛɛrɛw di minnu bɛ kɛ ka kɛɲɛ ni mɔgɔw sago ye walasa ka fɛn kɛrɛnkɛrɛnnenw wajibiyalenw dafa, ka baarakɛcogo ɲuman ni muɲuli sabati baara suguya caman na. Anw minnu ye silikɔni lastikuw dilabaga dannamɔgɔ ye, an bɛ fɛnw di minnu ka ɲi, minnu musaka ka dɔgɔ, minnu bɛ bɛn aw magow ma.


Silicone Rubber min bɛ kɛnɛya kosɛbɛ

GA-33×1 Silicone Rubber (Silicone fumed) (HCR) min bɛ kɛnɛya kosɛbɛ (HCR) - A jɔyɔrɔba


Transparence haute pour les applications claires

GA-33×1 silikɔni lastikuw dabɔra kɛnɛyakoba kama, o b’a to a dafalen don silikɔni lastikuw jɛlenw na. Nin fɛn in ka ɲi fɛnw ma i n’a fɔ dumunikɛminɛnw, sigilan jɛlenw, ani lastikuw jɛlen wɛrɛw, yɔrɔ minnu na jɛya ni fanga nafa ka bon. I mana kɛ furakɛli silikɔnifɛnw dilanni na wo, walima mɔgɔw ka fɛnw ye wo, nin silikɔni lastikuw bɛ kɛnɛyako sariyaw labato minnu ka bon kosɛbɛ.


Masina fanga ɲumanba

GA-33×1 bɛ masin fanga ɲuman di ani a bɛ se ka ɲɛji bɔ, o b’a to a ka ɲi kosɛbɛ baara la baara gɛlɛnw na. A bɛ kɛ kosɛbɛ lastikuw la minnu bɛ mɛn i n’a fɔ furakɛli sigilanw, mobili yɔrɔw, ani mɔgɔw ka fɛnw minnu ka kan ka baara kɛ ni dannaya ye waati kɔnɔ. O b’a kɛ sugandili ɲuman ye dilanbagaw bolo minnu bɛ silikoni lastikuw ɲini minnu fanga ka bon.


Baarakɛcogo ɲumanba

Nin silikɔni lastikuw min bɛ kɛnɛya kosɛbɛ, o bɛ baarakɛcogo ɲuman di, o bɛ kɛ sababu ye ka fɛnw ladilan nɔgɔya la walasa ka dilancogo mago kɛrɛnkɛrɛnnenw ɲɛ. I mana silikoni lastikuw yɔrɔ gɛlɛnw de wajibiya wo, walima a dilanni ka bon wo, GA-33×1 bɛ lastikuw dilanni nafama dɛmɛ ani silikɔni lastikuw furakɛcogo minnu bɛ kɛ ka kɛɲɛ ni i yɛrɛ sago ye. O bɛ fɛn dilanni waatiw ɲɛ ani ka dɛmɛ don ka fɛn dilanni musakaw dɔgɔya, o b’a kɛ fura ɲuman ye B2B jagokɛlaw bolo.


Duniya sariyaw labatoli

GA-33×1 silikɔni lastikuw bɛ bɛn diɲɛ lakana sariyakolo gɛlɛnw ma i n’a fɔ RoHS, REACH, ani LFGB. O seereyaw b’a jira ko a farati tɛ baara la iziniw na i n’a fɔ kɛnɛyako, dumuniko, ani ɛntɛrinɛti, o bɛ a to a ka ɲi kosɛbɛ lastikuw dilanni na. Dilanbagaw bɛ se ka da a la k’u ka fɛn dilannenw bɛ izini lakanani ni sigida laminiko wajibiyalenw dafa.


A ka ɲi kɛnɛyako ni mɔgɔw ka fɛnw na

Nin silikɔni lastikuw jɛlen in bɛ kɛ kɛnɛyako la kosɛbɛ, i n’a fɔ sinjiw ni den buteli sinjiw, ani fana mɔgɔw ka fɛnw na. A ka lakana sariyaw labatoli ani a ka kɛnɛyako ka bon, o b’a to a ye fɛn ye min ka di furakɛli silikɔni lastikuw ye. A ka ɲi fana ka lastikuw yɔrɔw dilan minnu bɛ kɛnɛya, minnu tɛ baga ye, minnu bɛ baara kɛcogo ɲuman ni lakana de wajibiya.


Funteni kunbɛnni sigida gɛlɛnw kama

GA-33×1 bɛ funteni kunbɛncogo ɲuman di, ka baarakɛcogo dafalen sabati sigidaw la minnu funteni ka bon kosɛbɛ. A kɛra funteni caman na wo, a kɛra funteni dɔgɔman ye wo, a b’a ka jogo mara, o b’a to a bɛnnen don ka baara kɛ ni mobili ye, silikɔni fɛnw na minnu bɛ se ka kɛ dumuni ye, ani furakɛli lastikuw yɔrɔw la minnu bɛ baara kɛ tuma bɛɛ cogoya gɛlɛnw na.


A tɛ baga ye ani a farati tɛ a kɛcogo la min bɛ se ka kɛ

Nin fɛn in tɛ baga ye, faritanabana tɛ a la, wa a farati tɛ ka kɛ a kɛcogo la min ka gɛlɛn. GA-33×1 bɛ diɲɛ lakana sariyaw labato, o b’a to a ka ɲi denmisɛnw ka fɛn dilannenw, furakɛli minɛnw ani fɛn wɛrɛw ma minnu bɛ mɔgɔ tɔɔrɔ. A dabɔra walasa a ka kɛ farati tɛ a tali la waati jan kɔnɔ kɛnɛyako ni dumuni nafamafɛnw na.


Aplikasi Range min bɛ se ka kɛ fɛn caman na

GA-33×1 silikɔni lastikuw bɛ kɛ baarakɛyɔrɔ caman na, i n’a fɔ mobili, furakɛli, mɔgɔw ka fɛnw ani ɛntɛrinɛti. A ka baarakɛcogo caman n’a ka baarakɛcogo ɲuman b’a kɛ sugandili dafalen ye jagokɛlaw bolo minnu bɛ silikɔni lamini furakɛlicogo jɛlenw ɲini minnu bɛ baara kɛ kosɛbɛ, minnu bɛ izini sariyaw dafa minnu ka gɛlɛn.


A ka silikɔni lastikuw furakɛcogo ladamulenw fɛ, a ka kɛnɛyako ka bon, ani a bɛ diɲɛ lakana sariyaw labato, GA-33×1 ye sugandili ye min bɛ da a kan jagokɛlaw bolo, minnu bɛ seko ni dɔnko siratigɛ la. I mana kɛ furakɛli silikɔnifɛnw dilanni na, mobili lastikuw yɔrɔw, walima mɔgɔw ka fɛnw, GA-33×1 bɛ silikɔni lastikuw di minnu bɛ mɛn, minnu bɛ kɛnɛya, min bɛ baarakɛcogo ni lakana sabatili sabati.


Ɲininkaliw ni jaabi minnu bɛ kɛ tuma caman na


J1: GA-33×1 silikɔni lastikuw min bɛ kɛnɛya kosɛbɛ, o nafa kunbabaw ye jumɛnw ye?
A1: GA-33×1 ka ɲi kosɛbɛ lastikuw yɔrɔ jɛlenw na i n’a fɔ sinjiw, furakɛli sigilanw, ani mɔgɔw ka fɛn jɛlenw.


J2: Yala GA-33×1 silikɔni lamini bɛ se ka kɛ ka kɛɲɛ ni baara kɛrɛnkɛrɛnnenw ye wa?
A2: Ɔwɔ, an bɛ silikɔni lamini furaw di minnu bɛ kɛ ka kɛɲɛ ni i ka dilancogo n’i ka baarakɛcogo magow ye.


J3: Yala GA-33×1 bɛ bɛn diɲɛ lakana sariyaw ma wa?
A3: Ɔwɔ, a bɛ RoHS, REACH, ani LFGB ka seereyaw dafa lakana siratigɛ la kɛnɛyako, dumuniko ani ɛntɛrinɛti kan.


J4: Baarakɛyɔrɔ jumɛnw de ka teli ka baara kɛ ni GA-33×1 silikɔni lastikuw ye?
A4: A bɛ kɛ kosɛbɛ kɛnɛyako, mobili, mɔgɔw ka fɛnw, ani ɛntɛrinɛti kan baarakɛcogo ɲumanw na.


J5: Yala GA-33×1 bɛ muɲuli ɲuman di funteni jugumanba kɔrɔ wa?
A5: Ɔwɔ, a bɛ se ka funteni caman ni funteni dɔgɔya, ka baara kɛcogo sabati cogoya gɛlɛnw na.


J6: Yala GA-33×1 tɛ baga ye wa a farati tɛ a kɛcogo la wa?
A6: Ɔwɔ, nin silikɔni lamini in tɛ baga ye, faritanabana tɛ a la, wa a farati tɛ furaw la minnu ka gɛlɛn i n’a fɔ sinjibɔlanw.


J7: GA-33×1 bɛ se ka suma cogo di ni silikɔni lamini jɛlen tɔw ye?
A7: GA-33×1 bɛ kɛnɛya, fanga ani baarakɛcogo ɲuman di baarakɛcogo gɛlɛnw ma.


J8: Yala GA-33×1 bɛ se ka kɛ dumunikɛminɛnw na wa?
A8: Ɔwɔ, a bɛ LFGB labato, wa a lakananen don dumuniko siratigɛ la, ka a to a ka ɲi ani ka a lakana.

Tɛmɛnen: 
Nata: 

LINKS TELIKANW

AN KA FƐƐRƐW

KUNNAFONIW MINNU BƐ SƆRƆ

A farala: No.33, Lane 159, Taiye sira kan, Fengxian mara la, Shanghai
Telefɔni / WhatsApp / Skype: +86 15221953351
Hakilila-jɔ-sɛbɛn     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap (yɔrɔ karti). |   Kunnafoni dogolenw ka sariya | Dɛmɛn By Leadong ye.