Maybe you are a SK purchasing manager, who are looking for high quality SK, and Herchy are a professional manufacturer & supplier that can meet your needs. Not only SK we produced have certificated the international industry standard, but we can also meet your customization needs. We provide online, timely service and you can get professional guidance on SK. Don't hesitate to get in touch with us if you are interested in SK, we won't let you down.
Appearance and condition: white (transparent or translucent) blocky Third monomer type and content: ENB, 2.3% Ethylene content: 57% Mooney viscosity: ML(1+4)125°C 35 Size: 25kg/block MOQ: 25kg