Katundu:
Kukana kutentha kwambiri (-20 ° C mpaka +250 ° C).
Kukana kwapadera kwa mafuta, mafuta, zosungunulira, ma asidi, ndi mabasi.
Kuthamanga kwakukulu kwamphamvu (10-20 MPa), kutsika kwapakati (<15% pa 150 ° C / 70h).
Cholepheretsa moto (mlingo wa UL94 V-0) ndi ozoni.
Ubwino:
Osakanizidwa kale ndi mankhwala (mwachitsanzo, bisphenol AF, peroxide) kuti awonongeke bwino.
Imasunga kukhazikika kwamphamvu m'malo opangira mankhwala.
Makalasi ogwirizana ndi FDA omwe amapezeka pazakudya/zachipatala.
Mapulogalamu:
Azamlengalenga: O-mphete zamafuta, zisindikizo za injini, ndi ma diaphragms.
Magalimoto: Ma gaskets a Turbocharger, zosindikizira zotumizira, ndi majekeseni amafuta.
Chemical: Zomangira pampu, mipando ya mavavu, ndi zomangira payipi.
Katundu:
Kukana kutentha mpaka +150 ° C (kwapakatikati + 175 ° C).
Kukana kwakukulu kwa mafuta, amines, ndi madzimadzi amadzimadzi.
Mphamvu zolimba kwambiri (15-35 MPa) komanso kukana kutopa.
Low permeability kwa mpweya.
Ubwino:
Pre-vulcanized kwa kuchepetsa processing nthawi.
Imasunga elasticity pansi pakuwonetsa kwanthawi yayitali ku media zankhanza.
Amapezeka m'makalasi a peroxide kapena sulfure.
Mapulogalamu:
Mafuta & Gasi: Zonyamula pobowola, zosindikizira zapampu zamatope, ndi zida zamutu.
Zagalimoto: Malamba anthawi, makina ojambulira mafuta, ndi mapaipi a turbocharger.
Industrial: Zisindikizo za silinda ya Hydraulic ndi zida za gearbox.
Katundu:
Kukana kwamafuta pang'ono (kuposa EPDM, kuchepera HNBR).
Kutentha kwapakati: -40°C mpaka +120°C.
Kukana kwakukulu kwa abrasion (ASTM D5963: 100-200 mm³ kutaya).
Kukhazikika kwabwino komanso kukana kwa compression set.
Ubwino:
Zotsika mtengo komanso zowoneka bwino kwambiri.
Customizable acrylonitrile content (18-50%) ya kukana mafuta ogwirizana.
Mapulogalamu:
Magalimoto: Mapaipi amafuta, mphete za O, ndi zisindikizo zotumizira.
Mafakitale: Malamba onyamula, zodzigudubuza, ndi zisindikizo zama hydraulic.
Ogula: Magolovesi a latex ndi zida zamasewera.
Katundu:
Kukaniza kwa ozoni / nyengo (maola 5,000+ pakuyesa kwa QUV).
Kutentha kwapakati: -50°C mpaka +150°C.
Mphamvu ya dielectric yapamwamba (20-30 kV/mm) ndi kusakwanira kwamadzi.
Low mpweya permeability.
Ubwino:
Opangidwa kale ndi antioxidants ndi UV stabilizers.
Kugwedera kwabwino kwambiri (chotayika: 0.1-0.3).
Mapulogalamu:
Magalimoto: Zisindikizo za zitseko, mapaipi a radiator, ndi zoyikira injini.
Kumanga: Zotchingira denga, zomangira dziwe, ndi gaskets zamawindo.
Zamagetsi: Kutsekereza ma chingwe ndi malamba otumizira mphamvu.
Katundu:
Kulimba kwamphamvu kwambiri (20-60 MPa) ndi kukhazikika (mpaka 800% elongation).
Kukana kwapadera kwa abrasion (ASTM D5963: 20-50 mm³ kutaya).
Kutentha kwamitundu: -40 ° C mpaka +100 ° C (mpaka +120 ° C ndi zowongolera kutentha).
Kugonjetsedwa ndi solvents ndi hydrolysis.
Ubwino:
Kuuma kosinthika (Shore A 50–95).
Amapezeka m'magalasi opangidwa ndi cast, millable, kapena thermoplastic.
Mapulogalamu:
Industrial: Mawilo, ma roller, ndi malamba onyamula katundu.
Zagalimoto: Zoyimitsidwa tchire, zotsekera zoziziritsa kukhosi, ndi nsapato za CV.
Zachipatala: Ma catheters, zingwe za mafupa, ndi ma prosthetics.
Katundu:
Kutentha kosalekeza mpaka +150 ° C (kwapakatikati + 175 ° C).
Kukana kwabwino kwamadzimadzi opatsirana (ATF), mafuta, ndi kutentha.
Ozone yokhazikika komanso kukana kwanyengo.
Mphamvu yamphamvu: 7-15 MPa.
Ubwino:
Osakanizidwa kale ndi mankhwala a amine kapena peroxide kuti achire mwachangu.
Imasunga kukhazikika m'malo a ATF.
Mapulogalamu:
Magalimoto: Zisindikizo zotumizira, mphete za O, ndi ma diaphragms opopera.
Zida zowongolera mphamvu zamagetsi.
Industrial: Pampu zosindikizira za media zotengera mafuta.
Katundu:
Kutentha kwakukulu (-40 ° C mpaka +150 ° C).
Kukana mafuta, glycols, ndi nyengo.
Kulimba kwamphamvu kwambiri (10-20 MPa) ndi kukana kwa seti ya compression.
Low permeability kwa mpweya.
Ubwino:
Imasinthasintha kukana kutentha ndi kusinthasintha.
Kugonjetsedwa ndi hydrolysis ndi kukalamba.
Amapezeka m'makalasi a peroxide kapena sulfure.
Mapulogalamu:
Magalimoto: Mapaipi a radiator, zida zoziziritsa kukhosi, ndi mapaipi olowera mpweya.
Mafakitale: Malamba onyamula mankhwala ndi ma diaphragms opopera.
HVAC: Ma duct gaskets ndi vibration isolator.