Ibyiza:
Kurwanya ubushyuhe bukabije (-20 ° C kugeza + 250 ° C).
Kurwanya bidasanzwe amavuta, ibicanwa, ibishishwa, acide, na base.
Imbaraga zikomeye (10–20 MPa), compression yo hasi (<15% kuri 150 ° C / 70h).
Flame retardant (UL94 V-0 igipimo) hamwe na ozone irwanya.
Ibyiza:
Byabanje kuvangwa nubuvuzi (urugero, bispenol AF, peroxide) kugirango ibirunga neza.
Igumana ihame ryimiterere yibidukikije byimiti.
Impamyabumenyi ya FDA iboneka kubiryo / kubonana n'abaganga.
Porogaramu:
Ikirere: Sisitemu ya lisansi O-impeta, kashe ya moteri, na diaphragms.
Imodoka: gasketi ya Turbocharger, kashe yohereza, hamwe ninshinge za lisansi.
Imiti: Amapompo, intebe za valve, hamwe ninteko ya hose.
Ibyiza:
Kurwanya ubushyuhe bugera kuri + 150 ° C (hagati + 175 ° C).
Kurwanya cyane amavuta, amine, hamwe na hydraulic fluid.
Imbaraga zikomeye (15-35 MPa) hamwe no kurwanya umunaniro.
Imyuka mike ya gaze.
Ibyiza:
Imbere-ibirunga kugirango bigabanye igihe cyo gutunganya.
Ikomeza gukomera mugihe kirekire itangazamakuru rikaze.
Biboneka muri peroxide- cyangwa sulfure-yakize amanota.
Porogaramu:
Amavuta na gazi: Abapakira, kashe ya pompe, nibice byiza.
Imodoka: Umukandara wigihe, sisitemu yo gutera lisansi, hamwe na shitingi ya turbocharger.
Inganda: Ikidodo cya Hydraulic kashe hamwe nibikoresho bya gearbox.
Ibyiza:
Kurwanya amavuta aringaniye (biruta EPDM, munsi ya HNBR).
Ubushyuhe: -40 ° C kugeza + 120 ° C.
Kurwanya cyane abrasion (ASTM D5963: 100-200 mm³ gutakaza).
Kwihangana neza no kwikuramo bishyiraho kurwanya.
Ibyiza:
Ikiguzi-cyiza hamwe nuburyo bwiza.
Guhindura ibintu bya acrylonitrile (18-50%) kubirwanya amavuta adasanzwe.
Porogaramu:
Imodoka: Amashanyarazi, O-impeta, hamwe na kashe yohereza.
Inganda: Imikandara ya convoyeur, imashini zandika, hamwe na kashe ya hydraulic.
Umuguzi: Gants ya Latex nibikoresho bya siporo.
Ibyiza:
Indwara ya ozone / ikirere cyiza (amasaha 5.000+ mugupima QUV).
Ubushyuhe: -50 ° C kugeza + 150 ° C.
Imbaraga nyinshi za dielectric (20-30 kV / mm) hamwe no kutagira amazi.
Umwuka wa gaze.
Ibyiza:
Byateguwe mbere na antioxydants na UV stabilisateur.
Kunyeganyega kwiza cyane (ikintu cyo gutakaza: 0.1–0.3).
Porogaramu:
Imodoka: Ikidodo cyumuryango, imashini yumuriro, hamwe na moteri.
Ubwubatsi: Ibisenge byo hejuru, ibizenga byamazi, hamwe na gaseke yidirishya.
Amashanyarazi: insinga ya insinga hamwe nimikandara yohereza amashanyarazi.
Ibyiza:
Imbaraga zikomeye (20-60 MPa) hamwe na elastique (kugera kuri 800%).
Kurwanya gukuramo bidasanzwe (ASTM D5963: 20-50 mm³ gutakaza).
Ubushyuhe: -40 ° C kugeza + 100 ° C (kugeza kuri + 120 ° C hamwe na stabilisateur).
Kurwanya kumashanyarazi na hydrolysis.
Ibyiza:
Gukomera gukomeye (Inkombe A 50–95).
Kuboneka muri cast, gusya, cyangwa amanota ya termoplastique.
Porogaramu:
Inganda: Ibiziga, ibizunguruka, n'umukandara wa convoyeur.
Automotive: Guhagarika bushing, imashini ikurura, hamwe na CV hamwe.
Ubuvuzi: Catheters, imitwe ya orthopedic, na prostate.
Ibyiza:
Gukomeza ubushyuhe bukabije kugeza kuri + 150 ° C (hagati + 175 ° C).
Kurwanya bihebuje kumashanyarazi yihuta (ATF), amavuta, nubushyuhe.
Gereranya ozone no guhangana nikirere.
Imbaraga zingana: 7-15 MPa.
Ibyiza:
Mbere-ivanze na amine cyangwa peroxide ivura kugirango ikire vuba.
Igumana ituze rinini mubidukikije bya ATF.
Porogaramu:
Imodoka: Ikimenyetso cyo kohereza, O-impeta, na pompe diaphragms.
Ibikoresho byo kuyobora sisitemu.
Inganda: Ikidodo cya pompe kubitangazamakuru bishingiye kuri peteroli.
Ibyiza:
Ubushyuhe bwagutse (-40 ° C kugeza + 150 ° C).
Kurwanya amavuta, glycol, hamwe nikirere.
Imbaraga zingana cyane (10–20 MPa) hamwe no kwikuramo gushiraho kurwanya.
Imyuka mike ya gaze.
Ibyiza:
Kuringaniza ubushyuhe no guhinduka.
Kurwanya hydrolysis no gusaza.
Biboneka muri peroxide- cyangwa sulfure-yakize amanota.
Porogaramu:
Imodoka: Amashanyarazi ya radiatori, ibice bya sisitemu ikonje, hamwe nu mwuka wo gufata umwuka.
Inganda: Imikandara ya convoyeur yo gukoresha imiti na pompe diaphragms.
HVAC: Umuyoboro wa gasketi hamwe na vibrateri ya vibrasiya.