Izakhiwo:
Ukumelana nokushisa ngokweqile (-20 ° C kuya ku-250 ° C).
Ukumelana okuhlukile kumafutha, amafutha, ama-solvents, ama-acid, nezisekelo.
Amandla aphezulu aphezulu (10-20 MPA), isethi yokucindezela ephansi (<15% ku-150 ° C / 70H).
I-Flame Retardant (UL94 V-0 Isilinganiso) kanye ne-Ozone-imelana ne-Ozone.
Izinzuzo:
Kuhlanganiswe kwangaphambilini ngama-curnatives (isib.
Igcina ukuqina kobukhulu ezindaweni ezinolaka kwamakhemikhali.
Amamaki avumelanayo we-FDA atholakala ngokudla / kokwelashwa.
Izicelo:
I-Aerospace: Uhlelo lwamafutha o-izindandatho, izimpawu zenjini, kanye nezichazamazwi.
Izithuthi: ama-gaskets e-turbocharger, izisuku zokuhambisa, kanye nemijovo kaphethiloli.
Amakhemikhali: ama-linlings wepompo, izihlalo ze-valve, kanye ne-hose assemblies.
Izakhiwo:
Ukumelana nokushisa kuze kufike ku- + 150 ° C (Intermittent + 175 ° C).
Ukumelana okuphezulu kumafutha, ama-Amines, kanye noketshezi lwe-hydraulic.
Amandla aphezulu aphezulu (15-35 MPA) nokuphikiswa ukukhathala.
Ukubheja okuphansi kumagesi.
Izinzuzo:
I-Pre-Vulkanized for isikhathi sokucisha okuncishisiwe.
Igcina ukuqina ngaphansi kokuvezwa isikhathi eside kwabezindaba ezinokhahlo.
Etholakala ePeroxide- noma amamaki aphelelwe ama-sulfur.
Izicelo:
Amafutha negesi: amaphakethe okumba, izimpawu zempompo zodaka, kanye nezingxenye ze-Wellhead.
Izithuthi: Amabhande wesikhathi, amasistimu wokujova kaphethiloli, nama-turbocharger hoses.
I-Industrial: Izimpawu zesilinda ze-hydraulic ne-hydraulic nezakhi zegiya.
Izakhiwo:
Ukumelana nowoyela okulinganiselwe (okungcono kune-EPDM, ngaphansi kwe-HNBR).
Ububanzi bokushisa: 40 ° C kuya ku-120 ° C.
Ukumelana ne-abrasion (ASTM D5963: Ukulahleka kwe-100-200 MM³).
Ukuqina okuhle nokuphikiswa kokuncipha.
Izinzuzo:
Kubiza kakhulu ukuphamba okuhle.
Okuqukethwe ngokwezifiso acrylonitrile okuqukethwe okwenziwe ngokwezifiso (18-50%) kokumelana namafutha enzelwe.
Izicelo:
Izithuthi: Ama-hoses ama-hoses, o-izindandatho, kanye nezimpawu zokudlulisa.
I-Industrial: Amabhande ahambisa, ama-roller wokuphrinta, kanye nezimpawu ze-hydraulic.
Umthengi: amagilavu we-latex kanye nemishini yezemidlalo.
Izakhiwo:
Ukumelana okuvelele kwe-Ozone / Isimo sezulu (amahora angama-5,000 + ekuhlolweni kwe-Quv).
Ububanzi bokushisa: -50 ° C kuya ku-150 ° C.
Amandla aphezulu we-dielectric (20-30 kv / mm) kanye nokungavikeleki kwamanzi.
Ukubheja okuphansi kwegesi.
Izinzuzo:
Kwakhiwa kuqala ngama-antioxidants kanye nama-UV aterilizer.
Ukudonswa okuhle kakhulu kwe-vibration (isici sokulahleka: 0.1-0.3).
Izicelo:
Izithuthi: Izibuko zomnyango, ama-radiator hoses, kanye nezintaba zenjini.
Ukwakha: Ulwelwesi oluphahla, ama-elond liners, nama-gaskets ewindi.
Electrical: Ukufakwa kwekhebula kanye namabhande okuhambisa amandla.
Izakhiwo:
Amandla aphezulu aphezulu (20-60 MPA) kanye nokuqina (kufika ku-800% elongation).
Ukumelana nokungafani kwe-abrasion (ASTM D5963: 20-50 MM³ ukulahleka).
Ububanzi bokushisa: 40 ° C kuya ku-100 ° C (kufika ku- + 120 ° C nge
Ukumelana nokuhlaziywa kanye ne-hydrolysis.
Izinzuzo:
Ubulukhuni ezenziwe ngezifiso (i-Shore A 50-95).
Kutholakala kumabanga aphonyisike, angaphansi, noma we-thermoplastic.
Izicelo:
Izimboni: amasondo, ama-roller, namabhande ehambisa.
Izithuthi: Izihlahla zokumiswa, ukuthuthumela kwama-hucock, kanye namabhuzu ahlanganyelwe we-CV.
Ezokwelapha: Ama-Catheters, ama-orthopedic brace, kanye nama-prosthetics.
Izakhiwo:
Ukumelana nokushisa okuqhubekayo kuze kufike ku- + 150 ° C (Intermittent + 175 ° C).
Ukumelana okuhle kakhulu kumanzi okuhambisa ngokuzenzakalelayo (i-ATF), oyela, nokushisa.
I-ozone ephakathi nendawo yokumelana nokumelana nesimo sezulu.
Amandla asheshayo: 7-15 MPA.
Izinzuzo:
Kuhlanganiswe kwangaphambili nge-amine noma i-peroxide curritives ukuze uphele ngokushesha.
Igcina ukuqina kobukhulu ezindaweni ze-ATF.
Izicelo:
Izithuthi: Izimpawu zokuhambisa, ama-O-Rings, kanye nePup Diaphragms.
Izingxenye zohlelo lokuqondisa amandla.
Izimboni: Izimpawu zepompo zemidiya esekelwe kawoyela.
Izakhiwo:
Ububanzi bokushisa obubanzi (40 ° C kuya ku-150 ° C).
Ukumelana namafutha, ama-glycols, kanye nesimo sezulu.
Amandla aphezulu aphezulu (10-20 MPA) kanye nokuvuselelwa kokuphikiswa.
Ukubheja okuphansi kumagesi.
Izinzuzo:
Ezilinganisweni ukumelana nokushisa nokuvumelana nezimo.
Ukumelana ne-hydrolysis kanye nokuguga.
Etholakala ePeroxide- noma amamaki aphelelwe ama-sulfur.
Izicelo:
Izithuthi: I-radiator hoses, izingxenye zohlelo olupholile, kanye nama-hoses wokudla komoya.
I-Industrial: Amabhande ahambisa amakhemikhali wokuphatha amakhemikhali kanye ne-pump diaphragms.
I-HVAC: Ama-gaskets we-Duct kanye ne-Vibration Iolators.