O mo: Gae » Ditšweletšwa » Motswako

Diraba tše di Kopantšwego: Dithoto tše di nago le Dintlha, Mehola le Ditirišo

1. Motswako wa FKM (FKM) .

Dithoto:

  • Kganetšo ya themperetšha ye e feteletšego (-20°C go ya go +250°C).

  • Kganetšo ye e kgethegilego ya oli, dibešwa, disolvent, diesiti, le metheo.

  • Matla a go goga a godimo (10-20 MPa), sete ya kgatelelo ya fase (<15% ka 150°C/70h).

  • Kgabo retardant (UL94 V-0 tekanyetso) le ozone-thibela.

Melemo: .

  • E hlakantšwe pele le dihlare tša go fodiša (mohlala, bisphenol AF, peroxide) bakeng sa vulcanization ye e šomago gabotse.

  • E boloka go tsepama ga dimenšene ka ditikologong tša dikhemikhale tše bogale.

  • Mephato yeo e obamelago FDA yeo e hwetšagalago bakeng sa go ikgokaganya le dijo/ka tša kalafo.

Dikgopelo: .

  • Sefofane: Di-O-ring tša tshepedišo ya makhura, ditiiso tša entšene le di- diaphragm.

  • Koloi: Di-gasket tša turbocharger, ditiiso tša phetišetšo le di- injector tša makhura.

  • Dikhemikhale: Di- lining tša pompo, ditulo tša di-valve le dikopano tša dihose.

2. Motswako wa HNBR (HNBR) .

Dithoto:

  • Kganetšo ya phišo go fihla go +150°C (go kgaotša +175°C).

  • Go ganetša mo go phagamego ga oli, di- amine le diela tša haeteroliki.

  • Phahameng tensile matla (15-35 MPa) le mokhathala ho hanyetsa.

  • Low permeability ho dikgase.

Melemo: .

  • Pre-vulcanized bakeng sa fokotswa tshebetso nako.

  • E boloka elasticity ka tlase ga go pepentšhwa ka nako e telele go methopo ya ditaba e thata.

  • E hwetšagala ka mephato yeo e fodišitšwego ka peroxide goba sebabole.

Dikgopelo: .

  • Oli & Gase: Diphuthelwana tša go phunya, ditiiso tša pompo ya leraga, le dikarolo tša hlogo ya sediba.

  • Koloi: Mabanta a nako, ditshepedišo tša go tsenya makhura le dihose tša turbocharger.

  • Industrial: Ditiiso tša silindara ya haeteroliki le dikarolo tša gearbox.

3. Motswako wa NBR (NBR) .

Dithoto:

  • Kganetšo ya oli ye e lekanetšego (e kaone go feta EPDM, ka fase ga HNBR).

  • Thempheretšha ya go fapana: -40°C go ya go +120°C.

  • Phahameng abrasion ho hanyetsa (ASTM D5963: 100-200 mm3 tahlehelo).

  • Good resilience le compression beha ho hanyetsa.

Melemo: .

  • Ditshenyagalelo-atlehang le moldability babatsehang.

  • Customizable acrylonitrile dikahare (18-50%) bakeng sa tailored oli ho hanyetsa.

Dikgopelo: .

  • Koloi: Dihose tša makhura, di-O-ring le ditiiso tša phetišetšo.

  • Diintaseteri: Mabanta a go sepetša, di-roller tša go gatiša le ditiiso tša haeteroliki.

  • Moreki: Diatlana tša latex le didirišwa tša dipapadi.

4. Motswako wa EPDM (Ethylene Propylene Diene Monomer) .

Dithoto:

  • Kganetšo ye e tšwetšego pele ya ozone / boemo bja leratadima (diiri tše 5,000+ ka diteko tša QUV).

  • Thempheretšha ya go fapana: -50°C go ya go +150°C.

  • Matla a phahameng a dielectric (20-30 kV / mm) le metsi impermeability.

  • Tlase khase permeability.

Melemo: .

  • Pre-formulated le antioxidants le UV stabilizers.

  • E babatsehang thothometsa damping (tahlehelo Ntlha: 0.1-0.3).

Dikgopelo: .

  • Koloi: Ditiiso tša mojako, dihose tša radiator le di- mount tša entšene.

  • Kago: Dimembrane tša go rulela, di- liner tša letamo le di- gasket tša mafasetere.

  • Motlakase: Cable kwahelang le matla phetiso mabanta.

5. Motswako wa MPU (MPU) .

Dithoto:

  • Matla a godimo a go goga (20-60 MPa) le elasticity (go fihla go 800% elongation).

  • Ikhethang abrasion ho hanyetsa (ASTM D5963: 20-50 mm3 tahlehelo).

  • Thempheretšha ya go fapana: -40°C go ya go +100°C (go fihla go +120°C ka di-stabilizer tša phišo).

  • E hanyetsa solvents le hydrolysis.

Melemo: .

  • Go thatafala mo go ka fetošwago (Shore A 50-95).

  • E hwetšagala ka mephato ya go tšhollwa, ya go šilwa goba ya polasetiki ya go fiša.

Dikgopelo: .

  • Intasteri: Maotwana, di-roller le mapanta a go sepetša.

  • Dikoloi: Dibushing tša go emiša, di-shock absorber le dibutšwana tša go kopanya CV.

  • Bongaka: Di- catheter, di- brace tša marapo le dilo tša maitirelo.

6. Motswako wa ACM (ACM) .

Dithoto:

  • Kganetšo ya phišo ye e tšwelago pele go fihla go +150°C (go kgaotša +175°C).

  • Kganetšo e botse kudu go diela tša phetišetšo ya go itiriša (ATF), dioli le phišo.

  • Ozone e lekanetšego le go ganetša boemo bja leratadima.

  • Matla a go goga: 7-15 MPa.

Melemo: .

  • E hlakantšwe pele le di-curative tša amine goba peroxide bakeng sa go fodiša ka lebelo.

  • E boloka go tsepama ga dimenšene ka ditikologong tša ATF.

Dikgopelo: .

  • Koloi: Ditiiso tša phetišetšo, di-O-ring le di- diaphragm tša pompo.

  • Matla go laola tsamaiso dikarolo.

  • Intasteri: Ditiiso tša pompo tša methopo ya ditaba ye e theilwego godimo ga oli.

7. Motswako wa AEM (AEM) .

Dithoto:

  • Wide thempereichara fapaneng (-40 ° C ho + 150 ° C).

  • Go ganetša oli, di- glycol le go fetoga ga boemo bja leratadima.

  • Phahameng tensile matla (10-20 MPa) le compression beha ho hanyetsa.

  • Low permeability ho dikgase.

Melemo: .

  • E lekalekanya go ganetša phišo le go fetofetoga le maemo.

  • E lwantšha hydrolysis le botšofadi.

  • E hwetšagala ka mephato yeo e fodišitšwego ka peroxide goba sebabole.

Dikgopelo: .

  • Koloi: Dihose tša radiator, dikarolo tša tshepedišo ya setšidifatši le dihose tša go tsenya moya.

  • Intasteri: Mabanta a go sepetša bakeng sa go swara dikhemikhale le di-diaphragm tša pompo.

  • HVAC: Di-gasket tša diphaephe le di-isolator tša go thothomela.


Dikgokagano tša ka pela .

Ditšweletšwa tša rena .

TSHEDIMOŠO YA KGOKAGANO

Add: No.33, Lane 159, Tsela ya Taiye, Setereke sa Fengxian, Shanghai
Mogala / WhatsApp / Skype: +86 15221953351
E-mail: .  info@herchyrubber.com
Tokelo ya ngwalollo e ileditšwe     2023 Shanghai Herchy Rabara Co., Ltd. Mmapa wa Sebaka |   Pholisi ya Sephiri | Thekgo Ka Leadong ..