Thil neih:
A lumna nasa tak (-20°C atanga +250°C thleng) a ni.
Oil, fuel, solvent, acid leh base te laka a invenna danglam tak.
Tensile chakna sang (10–20 MPa), compression set hniam (150°C/70h-a <15%) a ni.
Meialh laka invenna (UL94 V-0 rating) leh ozone laka invenna a ni.
A thatna:
Vulcanization tha tak neih theih nan curatives (eg, bisphenol AF, peroxide) nen pre-blended a ni.
Chemical environment nasa takah chuan dimensional stability a vawng reng thin.
FDA-compliant grades ei tur/medical contact atan a awm.
Dilna: 1.1.
Aerospace: Fuel system O-ring, engine seal leh diaphragm te.
Automotive: Turbocharger gasket, transmission seal, leh fuel injector te.
Chemical: pump linings, valve seat, leh hose assembly te.
Thil neih:
+150°C thlenga lum theihna (intermittent +175°C) thleng thei a ni.
Oil, amine leh hydraulic fluid te laka invenna tha zawk.
Tensile chakna sang (15–35 MPa) leh hahna do thei.
Gas-te laka permeability hniam tak.
A thatna:
Processing hun tihtlem nan pre-vulcanized a ni.
Media khauh takah hun rei tak a awm hnuah elasticity a vawng reng thin.
Peroxide- emaw sulfur-cured grade-ah pawh a awm.
Dilna: 1.1.
Oil & Gas: Drilling packers, mud pump seal, leh wellhead components te a awm a.
Automotive: timing belt, fuel injection system, leh turbocharger hose te.
Industrial: Hydraulic cylinder seal leh gearbox component hrang hrangte.
Thil neih:
Oil resistance tlemte (EPDM aiin a tha zawk, HNBR aiin a tlem zawk).
Temperature range: -40°C atanga +120°C thleng a ni.
Abrasion do theihna sang tak (ASTM D5963: 100–200 mm3 hloh).
Resilience tha leh compression set resistance.
A thatna:
A man tlawm a, moldability tha tak a nei bawk.
Oil laka invenna tur acrylonitrile awm zat (18–50%) chu a duh angin a siam theih.
Dilna: 1.1.
Automotive: Fuel hose, O-rings, leh transmission seal te.
Industrial: Conveyor belt, printing rollers, leh hydraulic seal te hman a ni.
Consumer: Latex gloves leh infiamna hmanrua.
Thil neih:
Ozone/weather resistance langsar tak (QUV test-naah darkar 5,000+).
A lumna hmun: -50°C atanga +150°C thleng a ni.
Dielectric chakna sang (20–30 kV/mm) leh tui awm lohna (water impermeability) a ni.
Gas permeability hniam tak a awm.
A thatna:
Antioxidants leh UV stabilizers hmanga siam hmasak a ni.
Vibration damping tha tak (loss factor: 0.1–0.3).
Dilna: 1.1.
Automotive: Kawngkhar seal, radiator hose, leh engine mount te.
A sak dan: Roofing membrane, pond liners, leh window gasket te.
Electrical: Cable insulation leh power transmission belt hmanga siam a ni.
Thil neih:
Tensile strength sang (20–60 MPa) leh elasticity sang tak (800% elongation thleng) a ni.
Abrasion do theihna danglam tak (ASTM D5963: 20–50 mm3 hloh).
Temperature range: -40°C atanga +100°C (+120°C thleng a ni a, a lumna stabilizers a awm bawk).
Solvent leh hydrolysis laka inven theih a ni.
A thatna:
Hardness chu a duh angin a siam theih (Shore A 50–95).
Cast, millable, emaw thermoplastic grade-ah te a awm thei.
Dilna: 1.1.
Industrial: wheel, rollers, leh conveyor belt te.
Automotive: Suspension bushings, shock absorbers, leh CV joint boots te.
Medical: catheter, orthopedic braces, leh prosthetics te.
Thil neih:
+150°C thlenga lumna do chhunzawm zel (intermittent +175°C).
Automatic transmission fluid (ATF), oil, leh lumna laka invenna tha tak a ni.
Ozone leh khaw lum leh khaw vawt laka invenna (moderate) a ni.
Tensile chakna: 7–15 MPa.
A thatna:
Amine emaw peroxide curatives emaw hmanga pre-blended a ni a, curing chak tak a ni.
ATF environment-a dimensional stability a vawng reng.
Dilna: 1.1.
Automotive: Transmission seal, O-ring, leh pump diaphragm te a awm bawk.
Power steering system hmanga siam a ni.
Industrial: Oil hmanga siam media atana pump seal siam.
Thil neih:
Temperature zau tak (-40°C atanga +150°C thleng).
Oils, glycols, leh weathering laka inven theihna.
Tensile chakna sang (10–20 MPa) leh compression set resistance sang tak a ni.
Gas-te laka permeability hniam tak.
A thatna:
Heat resistance leh flexibility a balance.
Hydrolysis leh tar chakna laka a do thei.
Peroxide- emaw sulfur-cured grade-ah pawh a awm.
Dilna: 1.1.
Automotive: Radiator hose, coolant system component hrang hrang, leh air intake hose te.
Industrial: Chemical hmanna tur conveyor belt leh pump diaphragm hmanna tur.
HVAC: duct gasket leh vibration isolators te a awm.