Rubbers ngwakọta: Njirimara zuru oke, uru na ngwa

1. Ngwakọta FKM (FKM)

Njirimara:

  • Nnukwu nguzogide okpomọkụ (-20°C ruo +250°C).

  • Nguzogide pụrụiche megide mmanụ, mmanụ ọkụ, ihe mgbaze, acids na ntọala.

  • Ike ike dị elu (10-20 MPa), obere mkpakọ setịpụrụ (<15% na 150 ° C / 70h).

  • Ọkụ retardant (UL94 V-0) na ozone na-eguzogide.

Uru:

  • Ejikọtara ya na curatives (dịka ọmụmaatụ, bisphenol AF, peroxide) maka ịgbachapụ nke ọma.

  • Na-ejigide nkwụsi ike na mpaghara kemịkalụ ike ike.

  • Ọkwa FDA kwadoro maka nri/kọntaktị ahụike.

Ngwa:

  • Aerospace: O-mgbanaka sistemụ mmanụ ụgbọala, akara injin, na diaphragms.

  • Automotive: Turbocharger gaskets, nnyefe akara, na mmanụ ụgbọala injectors.

  • Chemical: Ihe mkpuchi mgbapụta, oche valvụ, na mgbakọ mmiri.

2. Ngwakọta HNBR (HNBR)

Njirimara:

  • Okpomọkụ na-eguzogide ruo + 150 ° C (na-adịte aka + 175 ° C).

  • Iguzogide mmanụ, amines, na mmiri mmiri hydraulic dị elu.

  • Ike ike dị elu (15-35 MPa) na ike ọgwụgwụ.

  • Obere permeability na gas.

Uru:

  • Pre-vulcanized maka mbelata oge nhazi.

  • Na-ejigide ngbanwe n'okpuru mkpughe ogologo oge na mgbasa ozi siri ike.

  • Dị na peroxide- ma ọ bụ sọlfọ gwọrọ akara ule.

Ngwa:

  • Mmanụ & Gas: Ndị na-akwakọba ihe, ihe mkpuchi apịtị, na ihe isi mmiri.

  • Ụgbọala: eriri oge, sistemu ịgba mmanụ, na hoses turbocharger.

  • Ụlọ ọrụ mmepụta ihe: Hydraulic cylinder seals na gearbox components.

3. Ngwakọta NBR (NBR)

Njirimara:

  • Nguzogide mmanụ dị oke mma (dị mma karịa EPDM, ihe na-erughị HNBR).

  • Okpomọkụ dị nso: -40°C ruo +120°C.

  • Nnukwu nguzogide abrasion (ASTM D5963: mfu 100-200 mm³).

  • Ezi nkwụsi ike na mkpakọ setịpụrụ nguzogide.

Uru:

  • Ọnụ-dị irè na ezigbo moldability.

  • Ọdịnaya acrylonitrile nwere ike ịhazi (18-50%) maka nguzogide mmanụ ahaziri.

Ngwa:

  • Ụgbọala: Ọkụ mmanụ ụgbọala, O-mgbanaka, na akara nnyefe.

  • Ụlọ ọrụ mmepụta ihe: eriri ebufe, rollers na-ebi akwụkwọ, na akara hydraulic.

  • Onye na-eri ihe: uwe mkpuchi latex na akụrụngwa egwuregwu.

4. Ngwakọta EPDM (Ethylene Propylene Diene Monomer)

Njirimara:

  • Ozone/ ihu igwe pụtara ìhè (awa 5,000+ na ule QUV).

  • Okpomọkụ dị nso: -50°C ruo +150°C.

  • Ike dielectric dị elu (20-30 kV / mm) na enweghị ike mmiri.

  • Obere gas permeability.

Uru:

  • Emebere ya nke ọma na antioxidants na UV stabilizers.

  • Mmanya ịma jijiji mara mma (ihe na-efu: 0.1-0.3).

Ngwa:

  • Akụrụngwa: Akàrà ọnụ ụzọ, ọkpọkọ radiator, na igwe njin.

  • Ihe owuwu: mkpuchi mkpuchi ụlọ, akwa ọdọ mmiri, na gaskets windo.

  • Eletriki: Igwe mkpuchi eriri na eriri nnyefe ike.

5. Ngwakọta MPU (MPU)

Njirimara:

  • Ike ike dị elu (20-60 MPa) na elasticity (ruo 800% elongation).

  • Nguzogide abrasion pụrụiche (ASTM D5963: mfu 20–50 mm³).

  • Okpomọkụ dị nso: -40°C ruo +100°C (ruo +120°C nwere ihe nkwụsi ike ọkụ).

  • Na-eguzogide ihe mgbaze na hydrolysis.

Uru:

  • Isi ike nwere ike ịhazi ya (Oké Osimiri A 50–95).

  • Dị na nkedo, igwe igwe, ma ọ bụ akara thermoplastic.

Ngwa:

  • Ụlọ ọrụ mmepụta ihe: wiil, rollers, na eriri ebufe.

  • Ụgbọala: Nkwusioru nkwusioru, ihe na-awụ akpata oyi n'ahụ, na akpụkpọ ụkwụ nkwonkwo CV.

  • Ahụike: Catheters, ihe nkwado orthopedic, na prosthetics.

6. Ngwakọta ACM (ACM)

Njirimara:

  • Okpomọkụ na-aga n'ihu ruo +150°C (na-adịte aka +175°C).

  • Nguzogide dị oke mma maka mmiri nnyefe akpaaka (ATF), mmanụ na okpomọkụ.

  • Ozone na-agafeghị oke na nguzogide ihu igwe.

  • Ike nkwụsị: 7–15 MPa.

Uru:

  • Ejikọtara ya na amine ma ọ bụ peroxide curatives maka ọgwụgwọ ngwa ngwa.

  • Na-edobe nkwụsi ike akụkụ na gburugburu ATF.

Ngwa:

  • Ụgbọala: Akara nnyefe, O-mgbanaka, na diaphragms mgbapụta.

  • Akụrụngwa sistemu ike.

  • Ụlọ ọrụ mmepụta ihe: Mgbapụta mgbapụta maka mgbasa ozi dabeere na mmanụ.

7. Ngwakọta AEM (AEM)

Njirimara:

  • Okpomọkụ dị obosara (-40°C ruo +150°C).

  • Iguzogide mmanụ, glycols na ihu igwe.

  • Ike ike dị elu (10-20 MPa) na mkpakọ setịpụrụ nguzogide.

  • Obere permeability na gas.

Uru:

  • Na-edozi nguzogide okpomọkụ na mgbanwe.

  • Na-eguzogide hydrolysis na ịka nká.

  • Dị na peroxide- ma ọ bụ sọlfọ gwọrọ akara ule.

Ngwa:

  • Akpaaka: Ọkpụkpụ radieshọn, ihe mejupụtara sistemu oyi na-ekpo ọkụ, na sọks nnabata ikuku.

  • Ụlọ ọrụ mmepụta ihe: eriri na-ebugharị maka njikwa kemịkalụ na mgbapụta diaphragms.

  • HVAC: gaskets olulu na ihe ndị na-eme mkpọtụ.


Njikọ ngwa ngwa

Ngwaahịa anyị

OZI MKPỌTỤRỤ

Tinye: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Nwebiisinka     2023 Shanghai Herchy Rubber Co., Ltd. map saịtị |   Amụma nzuzo | Nkwado Site Leadong.