1. FKM Compound (FKM)

Katundu:

  • Kukana kutentha kwambiri (-20 ° C mpaka +250 ° C).

  • Kukana kwapadera kwa mafuta, mafuta, zosungunulira, ma asidi, ndi mabasi.

  • Kuthamanga kwakukulu kwamphamvu (10-20 MPa), kutsika kwapakati (<15% pa 150 ° C / 70h).

  • Cholepheretsa moto (mlingo wa UL94 V-0) ndi ozoni.

Ubwino:

  • Osakanizidwa kale ndi mankhwala (mwachitsanzo, bisphenol AF, peroxide) kuti awonongeke bwino.

  • Imasunga kukhazikika kwamphamvu m'malo opangira mankhwala.

  • Makalasi ogwirizana ndi FDA omwe amapezeka pazakudya/zachipatala.

Mapulogalamu:

  • Azamlengalenga: O-mphete zamafuta, zisindikizo za injini, ndi ma diaphragms.

  • Magalimoto: Ma gaskets a Turbocharger, zosindikizira zotumizira, ndi majekeseni amafuta.

  • Chemical: Zomangira pampu, mipando ya mavavu, ndi zomangira payipi.

2. HNBR Compound (HNBR)

Katundu:

  • Kukana kutentha mpaka +150 ° C (kwapakatikati + 175 ° C).

  • Kukana kwakukulu kwa mafuta, amines, ndi madzimadzi amadzimadzi.

  • Mphamvu zolimba kwambiri (15-35 MPa) komanso kukana kutopa.

  • Low permeability kwa mpweya.

Ubwino:

  • Pre-vulcanized kwa kuchepetsa processing nthawi.

  • Imasunga elasticity pansi pakuwonetsa kwanthawi yayitali ku media zankhanza.

  • Amapezeka m'makalasi a peroxide kapena sulfure.

Mapulogalamu:

  • Mafuta & Gasi: Zonyamula pobowola, zosindikizira zapampu zamatope, ndi zida zamutu.

  • Zagalimoto: Malamba anthawi, makina ojambulira mafuta, ndi mapaipi a turbocharger.

  • Industrial: Zisindikizo za silinda ya Hydraulic ndi zida za gearbox.

3. NBR Compound (NBR)

Katundu:

  • Kukana kwamafuta pang'ono (kuposa EPDM, kuchepera HNBR).

  • Kutentha kwapakati: -40°C mpaka +120°C.

  • Kukana kwakukulu kwa abrasion (ASTM D5963: 100-200 mm³ kutaya).

  • Kukhazikika kwabwino komanso kukana kwa compression set.

Ubwino:

  • Zotsika mtengo komanso zowoneka bwino kwambiri.

  • Customizable acrylonitrile content (18-50%) ya kukana mafuta ogwirizana.

Mapulogalamu:

  • Magalimoto: Mapaipi amafuta, mphete za O, ndi zisindikizo zotumizira.

  • Mafakitale: Malamba onyamula, zodzigudubuza, ndi zisindikizo zama hydraulic.

  • Ogula: Magolovesi a latex ndi zida zamasewera.

4. EPDM Compound (Ethylene Propylene Diene Monomer)

Katundu:

  • Kukaniza kwa ozoni / nyengo (maola 5,000+ pakuyesa kwa QUV).

  • Kutentha kwapakati: -50°C mpaka +150°C.

  • Mphamvu ya dielectric yapamwamba (20-30 kV/mm) ndi kusakwanira kwamadzi.

  • Low mpweya permeability.

Ubwino:

  • Opangidwa kale ndi antioxidants ndi UV stabilizers.

  • Kugwedera kwabwino kwambiri (chotayika: 0.1-0.3).

Mapulogalamu:

  • Magalimoto: Zisindikizo za zitseko, mapaipi a radiator, ndi zoyikira injini.

  • Kumanga: Zotchingira denga, zomangira dziwe, ndi gaskets zamawindo.

  • Zamagetsi: Kutsekereza ma chingwe ndi malamba otumizira mphamvu.

5. MPU Compound (MPU)

Katundu:

  • Kulimba kwamphamvu kwambiri (20-60 MPa) ndi kukhazikika (mpaka 800% elongation).

  • Kukana kwapadera kwa abrasion (ASTM D5963: 20-50 mm³ kutaya).

  • Kutentha kwamitundu: -40 ° C mpaka +100 ° C (mpaka +120 ° C ndi zowongolera kutentha).

  • Kugonjetsedwa ndi solvents ndi hydrolysis.

Ubwino:

  • Kuuma kosinthika (Shore A 50–95).

  • Amapezeka m'magalasi opangidwa ndi cast, millable, kapena thermoplastic.

Mapulogalamu:

  • Industrial: Mawilo, ma roller, ndi malamba onyamula katundu.

  • Zagalimoto: Zoyimitsidwa tchire, zotsekera zoziziritsa kukhosi, ndi nsapato za CV.

  • Zachipatala: Ma catheters, zingwe za mafupa, ndi ma prosthetics.

6. ACM Compound (ACM)

Katundu:

  • Kutentha kosalekeza mpaka +150 ° C (kwapakatikati + 175 ° C).

  • Kukana kwabwino kwamadzimadzi opatsirana (ATF), mafuta, ndi kutentha.

  • Ozone yokhazikika komanso kukana kwanyengo.

  • Mphamvu yamphamvu: 7-15 MPa.

Ubwino:

  • Osakanizidwa kale ndi mankhwala a amine kapena peroxide kuti achire mwachangu.

  • Imasunga kukhazikika m'malo a ATF.

Mapulogalamu:

  • Magalimoto: Zisindikizo zotumizira, mphete za O, ndi ma diaphragms opopera.

  • Zida zowongolera mphamvu zamagetsi.

  • Industrial: Pampu zosindikizira za media zotengera mafuta.

7. AEM Compound (AEM)

Katundu:

  • Kutentha kwakukulu (-40 ° C mpaka +150 ° C).

  • Kukana mafuta, glycols, ndi nyengo.

  • Kulimba kwamphamvu kwambiri (10-20 MPa) ndi kukana kwa seti ya compression.

  • Low permeability kwa mpweya.

Ubwino:

  • Imasinthasintha kukana kutentha ndi kusinthasintha.

  • Kugonjetsedwa ndi hydrolysis ndi kukalamba.

  • Amapezeka m'makalasi a peroxide kapena sulfure.

Mapulogalamu:

  • Magalimoto: Mapaipi a radiator, zida zoziziritsa kukhosi, ndi mapaipi olowera mpweya.

  • Mafakitale: Malamba onyamula mankhwala ndi ma diaphragms opopera.

  • HVAC: Ma duct gaskets ndi vibration isolator.


MALANGIZO OPHUNZITSA

ZOPHUNZITSA ZATHU

ZAMBIRI ZAMALUMIKIZIDWE

Onjezani: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Ufulu     2023 Shanghai Herchy Rubber Co., Ltd. Mapu atsamba |   Mfundo Zazinsinsi | Support By Leadong.