A lan dan leh a dinhmun: var (transparent emaw translucent emaw) blocky
Third monomer chi leh a awm zat: ENB, 8.5%
Ethylene awm zat: 60%
Mooney viscosity: ML(1+4)125°C 109
Size: 25kg/block
MOQ: 25kg
Packing: boxed