Tel: +86 15221953351 E-mail: info@herchyrubber.com
Please Choose Your Language
PRODUCTS THIL THAWN THAWN THIL THIL THIL THIL THIL THIL THIL THIL THIL THAWN
Hetah hian i awm: In » Thil siam chhuah te » Synthesis rubber 1000 a ni. » VMQ Silicone 1000 a ni. » GA-99XX Vapor Phase Silica tichaktu Low Compression Set Silicone Rubber (HCR)

Loading a awm em?

Share to:
Facebook Sharing button a awm bawk.
twitter hmanga share theih a ni
Line Sharing button a awm bawk.
WeChat hmanga Sharing tih a ni.
LinkedIn Sharing button a awm bawk.
Pinterest hmanga Sharing tih a ni.
WhatsApp Sharing button 1000 a awm bawk.
ShareHe Sharing button hi a awm em?

GA-99xx vapor phase silica tihchakna compression hniam tak set silicone rubber (HCR)

Vapor phase silica tihchakna silicone rubber。
A hman dan: auto parts, heat-resistant cots, heat-resistantseals leh thil dang siamna atan a tha.
Thil pawimawh tak tak: heat「esistance tha leh mechanical strength, RoHS, REACH, leh FDA te authentication pass.
  • GA-99XX-ah a awm

  • Herchy a ni

A awm theihna:
A zat:

GA-99xx vapor phase silica tihchakna compression hniam tak set silicone rubber (HCR)


A hman dan: sealing ring, cots, auto parts leh otherproducts siamna atan a tha.
A pawimawh ber chu: resilience sang, compression set hniam, non-toxic tasteless HSE, RoHS, REACH leh FDA te authentication pass.
Test: Curing agent 1% (silicone gum-a DBPMH paste 50%), 175心5minx 15MPa.


Product Parameters 1000 a ni.

Thilsiam GA-9930 hmanga tih a ni GA-9935H a ni GA-9935 hmanga tih a ni GA-9940 hmanga tih a ni GA-9950 hmanga tih a ni GA-9960 hmanga tih a ni GA-9970T hmanga siam a ni
Landan Translucent 1000 a ni. Milky White a ni Translucent 1000 a ni.
Williamplasticity . 120 140 130 140 160 200 250
Harsatna (Shorea) . 30 33 36 40 50 60 70
Density(g/cm3) a ni. 1.1 1.1 1.1 1.11 1.12 1.15 1.17
Tensile chakna (MPA) . 7 9.5 9.5 8 9 9 9.5


A sei zawng(%) . 700 800 700 600 400 300 250
Tear chakna (kn/m) . 15 15 15 15 20 20 20
175'C x22h Compression(%) a ni. 15 20 15 15 15 15 15


Hma chiah: 
Dawtchiah: 

QUICK LINKS A AWM VE ANG

Contact information te .

Add: No.33, Lane 159, Taiye kawngpui, Fengxian District, Shanghai-a awm a ni
Tel / WhatsApp / Skype: +86 15221953351 ah zawhfiah theih a ni
E-mail hmangin:  info@herchyrubber.com
A rilru a hah   lutuk chuan a rilru   2023 a buai em em a. Shanghai Herchy Rubber Co., Ltd. Sitemap a ni |   Thuruk humhalh dan tur | Support By Leadong a ni.