Thil neih:
A lumna a nasa lutuk (-20°C atanga +250°C thleng).
Oil, fuel, solvent, acid leh base te laka invenna danglam tak.
Tensile chakna sang (10–20 MPa), compression set hniam (150°C/70H-ah <15%).
Flame retardant (UL94 V-0 rating) leh ozone-resistant te an ni.
A thatna:
Vulcanization tha tak neih theih nan curatives (eg, bisphenol AF, peroxide) hmanga pre-blended a ni.
Chemical boruak na tak karah dimensional stability a vawng reng.
FDA-compliant grades ei tur/medical contact atan a awm.
Dilna: 1.1.
Aerospace: Fuel system O-ring, engine seal leh diaphragm te.
Automotive: Turbocharger gasket, transmission seal, leh fuel injector te.
Chemical: pump linings, valve seat, leh hose assembly te.
Thil neih:
+150°C thlenga lum theihna (intermittent +175°C) thleng thei a ni.
Oil, amine leh hydraulic fluid te laka invenna tha zawk.
Tensile chakna sang (15–35 MPa) leh hahna do thei.
Gas-te tana permeability hniam.
A thatna:
Processing hun tihtlem nan pre-vulcanized a ni.
Media na tak tak nena hun rei tak an hman theih avangin elasticity a vawng reng thin.
peroxide- emaw sulfur-cured grade-ah te pawh a awm thei.
Dilna: 1.1.
Oil & Gas: Drilling packers, mud pump seals, leh wellhead component te.
Automotive: timing belt, fuel injection system, leh turbocharger hose te.
Industrial: Hydraulic cylinder seal leh gearbox component hrang hrangte.
Thil neih:
Oil resistance tlem (EPDM aiin a tha zawk, HNBR aiin a tlem zawk).
A lumna hmun: -40°C atanga +120°C thleng a ni.
Abrasion do theihna sang (ASTM D5963: 100–200 mm³ hloh).
Resilience tha leh compression set resistance.
A thatna:
Cost-effective leh moldability tha tak a nei bawk.
Acrylonitrile awm zat (18–50%) chu a duh angin a siam theih a, chu chu oil resistance a ni.
Dilna: 1.1.
Automotive: Fuel hose, O-rings, leh transmission seal te.
Industrial: Conveyor belt, printing rollers, leh hydraulic seal te.
Consumer: Latex gloves leh infiamna hmanrua.
Thil neih:
Ozone/weather resistance langsar tak (QUV test-naah darkar 5,000+).
A lumna hmun: -50°C atanga +150°C thleng a ni.
Dielectric chakna sang (20–30 kV/mm) leh tui awm lohna (water impermeability) a ni.
Gas permeability hniam tak a awm.
A thatna:
Antioxidant leh UV stabilizer hmanga siam pre-formulated a ni.
Vibration damping tha tak (loss factor: 0.1–0.3).
Dilna: 1.1.
Automotive: Kawngkhar seal te, radiator hose te, leh engine mount te.
In sak dan: Inchung lam membrane, pond liners, leh window gasket te.
Electrical: Cable insulation leh power thawn chhuahna belt te.
Thil neih:
Tensile chakna sang (20–60 MPa) leh elasticity (800% elongation thleng) a ni.
Abrasion do theihna danglam bik (ASTM D5963: 20–50 mm³ hloh).
Temperature range: -40°C atanga +100°C (+120°C thleng a ni a, a lumna stabilizers a awm bawk).
Solvent leh hydrolysis laka inven theih a ni.
A thatna:
Hardness siam danglam theih (shore a 50–95).
Cast, millable, emaw thermoplastic grade-ah te a awm thei.
Dilna: 1.1.
Industrial: wheel, rollers, leh conveyor belt te.
Automotive: Suspension bushings, shock absorbers, leh CV joint boots te.
Medical: catheter, orthopedic braces, leh prosthetics te.
Thil neih:
+150°C thlenga lumna a thlen chhunzawm zel theih (intermittent +175°C) a ni.
Automatic transmission fluids (ATF), oils, leh heat te laka invenna tha tak a ni.
Ozone leh khaw lum leh khaw vawt laka inven theihna a awm.
Tensile chakna: 7–15 MPa.
A thatna:
Amine emaw peroxide curatives emaw hmanga pre-blended a ni a, curing chak tak a ni.
ATF environment-a dimensional stability a vawng reng.
Dilna: 1.1.
Automotive: Transmission seal, O-ring leh pump diaphragm te.
Power steering system hmanga siam a ni.
Industrial: Oil-based media-a hman tur pump seal te.
Thil neih:
A lumna hmun zau tak (-40°C atanga +150°C) a ni.
Oils, glycols, leh weathering laka inven theihna.
Tensile chakna sang (10–20 MPa) leh compression set resistance.
Gas-te tana permeability hniam.
A thatna:
Heat resistance leh flexibility a balance thei.
Hydrolysis leh aging laka inven theih a ni.
peroxide- emaw sulfur-cured grade-ah te pawh a awm thei.
Dilna: 1.1.
Automotive: Radiator hose, coolant system components, leh air intake hose te a awm bawk.
Industrial: Chemical hmanna tur conveyor belt leh pump diaphragms te.
HVAC: duct gasket leh vibration isolators te a awm.