Good Processability High Strength Hose Fluoroelastomer
Color: black
Vulcanization system: bisphenol system
Hardness: 70±5 SHORE A
Mooney viscosity: ML(1+10)121℃ 50-70
Size specification: can be more customized (sheet)
Vulcanization conditions: 175℃*10min Secondary vulcanization: 200℃*4h (2mm standard test piece)
Minimum order quantity: 50kg