Ku Endliwa Ka kahle Hose ya Matimba ya le Henhla Fluoroelastomer
Muhlovo: wa ntima
Sisiteme ya vulcanization: sisiteme ya bisphenol
Ku tiya: 70±5 SHORE A
Ku tsindziyela ka Mooney: ML(1+10)121°C 50-70
Ku hlamuseriwa ka vukulu: swi nga endliwa ngopfu hi ku landza swilaveko swa wena (phepha)
Swiyimo swa vulcanization: 175°C*10min Vulcanization ya vumbirhi: 200°C*4h (2mm standard test piece)
Minimum order nhlayo: 50kg