I-Rubber esebenzayo i-ejenti eyaziwa nangokuthi i-Vulcanizing agent esebenzayo. Into engaphakathi noma ye-organic esetshenziselwa ukwenza i-accelerator ye-vulcanization isebenze. Ingakhulisa umthamo we-accelerator, yehlise inani le-accelerator, futhi linciphise isikhathi sokuvuselela. Iningi lezengezo ze-inorganic liyi-oxides yensimbi, ama-hydroxides kanye ne-carbonates eyisisekelo, njenge-zinc onide, i-calcium hydroxive, i-calbonate aphine, i-njr, i-antine ejwayelekile, i-zinc stearate, njll. I-General DOSAGE ingaphansi kwe-5% yesisindo werabha.

Izithasiselo zeRubber: Izakhiwo ezinemininingwane, izinzuzo, kanye nezinhlelo zokusebenza

1. UZinc oxide (zno)

Izakhiwo:

  • I-White, i-Powder enephunga elinamakhaza aphezulu adonsela phansi (5.6 g / cm³).

  • Iphuzu elincibilikayo: 1,975 ° C; I-Index Resuactive: 2.008-2.029.

  • Ukuvuselelwa okuphezulu njengesishoseli se-vulcanization.

  • Ukuvinjwa kwe-UV kanye nezakhiwo ze-antimicrobial.

Izinzuzo:

  • Isheshisa i-Sulfur Vulcanization (inciphisa isikhathi sokuvuka ngo-20-30%).

  • Kuthuthukisa izakhiwo zemishini (amandla ashubile + 15-25%, ukusunduza ekhefu + 10-15%).

  • I-FDA-ivunyelwe izinhlelo zokusebenza zokuxhumana nokudla (21 CFR 172.480).

  • Imvelo inobungane (okungelona ubuthi, iphinde isebenze kabusha).

Izicelo:

  • Amathayi: Izidumbu ze-radio ezinsimbi ezingenantambo zensimbi (zithuthukisa ukunamathela phakathi kwenjoloba nensimbi).

  • Izicathulo zezinyawo: Amakhompiyutha okuphuma (athuthukisa ukumelana ne-abrasion, i-ASTM D5963: 50-80 MM³ ukulahleka).

  • Medical: Gloves ehlinchlizeni (Ukuvikelwa kwe-antimicrobial, ASTM E2149).

  • Adhesives: Bonding enjoloba (kukhulisa amandla we-peel ngo-30- 40%).

2. Phenolic resin

Izakhiwo:

  • I-Thermosetting polymer enobunzima obuphezulu be-crosslink.

  • Ukumelana nokushisa: Sebenzisa okuqhubekayo kuze kufike ku-180 ° C (Intermittent 250 ° C).

  • Ubulukhuni obuphakeme (modulus: 2-4 GPA) nokuqina okuyisici.

  • Ukumelana kwamakhemikhali kuma-acid, izisekelo kanye nama-solvents.

Izinzuzo:

  • Inikeza ukuqiniswa kwesakhiwo (kwandisa ubunzima ngo-10-20 Shore a).

  • I-Flame Retardant (UL94 V-0 Isilinganiso ngaphandle kwe-Halogen AddItives).

  • Kubiza kakhulu uma kuqhathaniswa nama-thermoplastics akhethekile.

  • Izinhlelo ezenziwe ngokwezifiso zokwelapha (i-acid-catalyzed noma isebenze ukushisa).

Izicelo:

  • Amathayi: Ama-Sidewall Compounds (athuthukisa ukumelana, i-ASTM D624).

  • Amabhande ezimboni: Amabhande ahambisa izimboni zezindawo eziphakeme zokushisa (isib. Izitshalo zikasimende).

  • Izinto zokungqubuzana: ama-brake pads (agcina i-coefficing yokushayela ku-0.35-0.45 ngaphansi kwama-200 ° C).

  • I-Fedry: Ama-Binders Sand Core (anciphisa ukuziphendukela kwemvelo kwegesi ngesikhathi sokuphosa).


Izixhumanisi ezisheshayo

Imikhiqizo yethu

ULWAZI LOKUXHUMANA

Faka: Cha.33, Umzila 159, Taiye Road, Fenghian District, Shanghai
I-TEL / WhatsApp / Skype: +86 15221953351
I-imeyili:  info@herchyrubber.com
I-copyright     2023 Shanghai Herchy Rubber Co, Ltd. Indawo lapho ittamap |   Inqubomgomo Yobumfihlo | Ukusekelwa ngu Govong.