Izakhiwo:
Ukumelana nezinga lokushisa okwedlulele (-20°C kuya +250°C).
Ukumelana okukhethekile nowoyela, amafutha, izincibilikisi, ama-asidi, nezisekelo.
Amandla aqine kakhulu (10–20 MPa), isethi yokucindezela okuphansi (<15% ku-150°C/70h).
I-flame retardant (isilinganiso se-UL94 V-0) futhi imelana ne-ozone.
Izinzuzo:
Ihlanganiswe ngaphambili nezinto zokwelapha (isb., i-bisphenol AF, i-peroxide) ukuze i-vulcanization ephumelelayo.
Igcina ukuqina kwe-dimensional ezindaweni zamakhemikhali ezinolaka.
Amamaki athobela i-FDA atholakalela ukudla/ukuxhumana nodokotela.
Izicelo:
I-Aerospace: Ama-O-rings wesistimu yesibaseli, izimpawu zenjini, nama-diaphragms.
Izimoto: I-Turbocharger gaskets, ama-transmission seal, nama-injection kaphethiloli.
I-Chemical: Amapayipi amapayipi, izihlalo zama-valve, nama-hose assemblies.
Izakhiwo:
Ukumelana nokushisa kuze kufike ku-+150 ° C (isikhashana +175 ° C).
Ukumelana okuphezulu nowoyela, ama-amine, noketshezi olunamanzi.
Amandla aphezulu okudonsa (15–35 MPa) kanye nokumelana nokukhathala.
Ukungena kancane kumagesi.
Izinzuzo:
I-pre-vulcanized ukuze inciphise isikhathi sokucubungula.
Igcina ukunwebeka ngaphansi kokuchayeka isikhathi eside kwabezindaba ezinokhahlo.
Itholakala nge-peroxide- noma amamaki e-sulfur-cured.
Izicelo:
Uwoyela Negesi: Izipakishi zokumba, izigxivizo zephampu yodaka, nezingxenye ze-wellhead.
Ezezimoto: Amabhande esikhathi, amasistimu omjovo kaphethiloli, namapayipi e-turbocharger.
Imboni: Izigxivizo ze-Hydraulic cylinder kanye nezingxenye ze-gearbox.
Izakhiwo:
Ukumelana nowoyela okumaphakathi (okungcono kune-EPDM, ngaphansi kwe-HNBR).
Ibanga lokushisa: -40°C ukuya +120°C.
Ukumelana nokuhuzuka okuphezulu (i-ASTM D5963: ukulahlekelwa okungu-100–200 mm³).
Ukuqina okuhle nokumelana nesethi yokucindezela.
Izinzuzo:
Ibiza kakhulu futhi inokubumba okuhle kakhulu.
Okuqukethwe kwe-acrylonitrile okwenziwe ngokwezifiso (18-50%) kokumelana nowoyela ofanelana nawe.
Izicelo:
Izimoto: Amapayipi kagesi, ama-O-rings, nama-transmission seal.
Imboni: Amabhande okuthutha, amarola okuphrinta, nama-hydraulic seal.
Umthengi: Amagilavu e-latex nemishini yezemidlalo.
Izakhiwo:
Ukumelana ne-ozone/isimo sezulu okuvelele (amahora angu-5,000+ ekuhlolweni kwe-QUV).
Ibanga lokushisa: -50°C kuya +150°C.
Amandla e-dielectric aphezulu (20–30 kV/mm) nokungangeni kwamanzi.
Ukungena kwegesi okuphansi.
Izinzuzo:
Yakhelwe ngaphambilini ngama-antioxidants nama-UV stabilizers.
Ukudambisa ukudlidliza okuhle kakhulu (isici sokulahlekelwa: 0.1–0.3).
Izicelo:
Izimoto: Izivalo zezicabha, amapayipi erediyetha, nezixhumi zenjini.
Ukwakhiwa: Ama-membrane okufulela, ama-pond liners, nama-gaskets amafasitela.
Ezogesi: Izintambo zokuvala amakhebula namabhande okudlulisa amandla.
Izakhiwo:
Amandla aqinile aphezulu (20-60 MPa) kanye nokunwebeka (kufika ku-800% ubude).
Ukumelana nokuhuzuka okukhethekile (i-ASTM D5963: ukulahlekelwa okungu-20–50 mm³).
Ibanga lokushisa: -40°C kuya ku-+100°C (kufika ku-+120°C ngeziqinisi lokushisa).
Ukumelana ne-solvents kanye ne-hydrolysis.
Izinzuzo:
Ubulukhuni obenziwa ngokwezifiso (Shore A 50–95).
Itholakala ku-cast, millable, noma amamaki e-thermoplastic.
Izicelo:
Imboni: Amasondo, amarola, namabhande okuthutha.
Izimoto: Izihlahla ezimisiwe, izinto zokudonsa ama- shock, namabhuzu ahlangene e-CV.
Ezokwelapha: Ama-catheter, ama-orthopedic braces, kanye ne-prosthetics.
Izakhiwo:
Ukumelana nokushisa okuqhubekayo kufika ku-+150 ° C (isikhashana +175 ° C).
Ukumelana okuhle kakhulu noketshezi oluzenzakalelayo lokudlulisela (ATF), uwoyela, nokushisa.
I-ozone emaphakathi nesimo sezulu.
Amandla okuqina: 7–15 MPa.
Izinzuzo:
Ihlanganiswe kusengaphambili nemithi yokwelapha i-amine noma i-peroxide ukuze ilapheke ngokushesha.
Igcina ukuzinza kwe-dimensional ezindaweni ze-ATF.
Izicelo:
Izimoto: Izimpawu zokudlulisa, ama-O-rings, nama-diaphragm epompo.
Izingxenye zesistimu yokuqondisa amandla.
Imboni: Izigxivizo zephampu zemidiya esekwe kuwoyela.
Izakhiwo:
Izinga lokushisa elibanzi (-40°C kuya ku-+150°C).
Ukumelana namafutha, ama-glycols, kanye nesimo sezulu.
Amandla aqinile aphezulu (10–20 MPa) kanye nokumelana nesethi yokucindezela.
Ukungena kancane kumagesi.
Izinzuzo:
Ibhalansisa ukumelana nokushisa nokuvumelana nezimo.
Imelana ne-hydrolysis nokuguga.
Itholakala nge-peroxide- noma amamaki e-sulfur-cured.
Izicelo:
Izimoto: Amapayipi erediyetha, izingxenye zesistimu ezipholile, namapayipi okungenisa umoya.
Imboni: Amabhande okuthutha okuphatha amakhemikhali kanye nama-diaphragm epompo.
I-HVAC: Ama-duct gaskets nezihlukanisi zokudlidliza.