Ntlafatsa nako ea nako ea boronse ea rabara

Ka linako tse ling basebelisi ba ka botsa feela hore na komporo e mpe e ka huloa nako e kae ntle le ho robeha. Ena ke thepa e 'ngoe ea bohlokoa tsa lintho tse bonahalang tse maemong a khatello ea maikutlo a khatello ea maikutlo a maemo a tloaelehileng joalo ka ha ho boletsoe ke Astm le Iso. Li-protocol tse latelang li ka thusa liforomo ho kopana le litlhoko tsa mosebelisi.

1. SBR

SBB e kenelletsoe ke emulsion ho -10 ° C ho fapana le ho 50 ° C

2. Nr

Har'a lipere tse fapaneng tsa NR, rabara ea tlhaho ea CV60 e na le ts'ebetso ea nako e telele e futhumetseng ka ho fetisisa.

3. Neoprene le lifilimi

Mefuteng ea Neoprene, lifilimi tsa antirgan li na le boholo bo boholo ho fapana le boholo bo fokolang ho fapana le boholo bo fokolang bo lokelang ho sebelisoa ho ntlafatsa nako ea khefu ea nako. Ntle le moo, ho fetola carbon e matlafalitsoeng kapa e matlafalitsoeng e ntšo e nang le carbon e chesang e ka ntlafatsang nkhono oa khefu ea nako.

4. Tpe le TPV

Li-Elastors tsa Thermoplane le Thermoplane le li-Elastomers tse nang le litlolo tse phahameng tsa li-elate tsa li-elate tse phahameng, moo matla a ho atleha le a mashome a mane a itšetlehileng ka oona.

5. Carbon e ntšo

Ts'ebeliso ea carbon e ntšo e nang le sebaka se tlase le sebopeho se tlase le palo e tlase ea ho tlatsa carbon e se nang carbon e ka ntlafatsa molumo oa motsoako oa komporo.

6. Talcum Powder

Pheta palo e lekanang ea khabone e ntšo e nang le visa e nyane e ka ntlafatsang ntlafatso ea motsoako, empa e ka eketsa Modulus matla a tlase mme a ka eketsa modulus ka bongata.

7. Sulfur Vulcanization

Monyetla o ikhethang oa sebaboko o bapisoang le Vulcanization ea peroxide ke hore e ka etsa hore lingoliloeng tsa rabara li be le nako e phahameng ea tensile. Ka kakaretso, litsamaiso tse phahameng tsa li-vilul tse phahameng li ka fana ka nako e ntle e ntle ea nako e ntle ea litsietsi ho feta litsamaiso tsa Sulfur tse tlase.

8. Gel

Moralo oa synthetic joaloka sbr ka kakaretso e na le likhahla. Leha ho le joalo, kopanya mekhahlelo ea SBR ka holim'a 163 ° C e ka hlahisa li-gels tse lokolotsoeng (tse ka phatloha ka li-geld tse bulehileng 'me li sa qheleloe ka li-solvents tse itseng). Li-gels ka bobeli li fokotsa nako ea nako ea komporo, kahoo mocheso o kopanyang oa SBR o lokela ho tšoaroa ka hloko.

9. Ho kopanya

Ho kopanya ho ntlafatsa ho hasana ha carbon e ntšo, e thusang ho ntlafatsa nako ea nako ea koluoa.

10. Liphello tsa boima ba limolek'hule

Bakeng sa bebe ea NBR e tala, tšebeliso ea lintho tse tlase tsa molengyy le boima ba limok'hulek'hule tse tlase li ka ntlafatsang nako ea nako ea khefu ea nako. Emulsion SBR, ssebed e qhibiliha, sbr, BR le I Ir le tsona li loketse sena.

11. Tekanyo ea Vulcanization

Ka kakaretso, ho ba le tekanyo e tlase ea ho ruruha ho ka lebisa ho nako e telele e teteaneng ea setsi seo.


Lihokela tse potlakileng

Lihlahisoa tsa rona

MOKHOA OA PUISANO

Kenya: No.33, Lane 159, Taiye Business, Setereke sa Fengxian, Shanghai
Tel / Whatsapp / Skype: + 86 15221953351
Copyright     2023 Shanghai Herchy Rubber Co, Ltd. Sitemap |   Leano la Lekunutu | Ts'ehetso ea Phelana.