Appearance and condition: white (transparent or translucent) blocky Third monomer type and content: ENB, 4.6% Ethylene content: 57.2% Oil charge: 20% Mooney viscosity: ML (1+4) 125°C 60 Size: 25kg/bag MOQ: 25kg Packing: boxed
Appearance and condition: Beige or pale yellow blocky Third monomer type and content: ENB, 8.9% Ethylene content: 60.1% Mooney viscosity: ML(1+4)100°C 64 Size: 25kg/block MOQ: 25kg Packing: boxed
Appearance and condition: Beige or pale yellow blocky Third monomer type and content: ENB, 4.4% Ethylene content: 68.6% Mooney viscosity: ML(1+4)125°C 60 Size: 25kg/block MOQ: 25kg Packing: boxed
Appearance and condition: Beige or pale yellow blocky Third monomer type and content: ENB, 8.5% Ethylene content: 52.5% Mooney viscosity: ML(1+4)125°C 68 Oil content:20% Size: 25kg/block MOQ: 25kg Packing: boxed