756
Mtengo wa magawo SABIC
Chithunzi cha SABIC EPDM756
| Kupezeka: | |
|---|---|
| Kuchuluka: | |
MFUNDO ZOYENERA KUCHITA:
| ZINTHU | MFUNDO ZOYENERA | MALANGIZO | NJIRA ZOYESA |
| ZINTHU ZA POLYMER | |||
| Kukhuthala kwa Mooney | |||
| ML 1+4, 125 °C (1) | 72 |
MU |
Chithunzi cha ASTMD 1646 |
| Zinthu za Ethylene | 69 |
wt.% |
Mtengo wa ASMD3900 |
| Ethylidene Norbornene (ENB) Zomwe zili | 5 |
wt.% | Chithunzi cha ASTMD6047 |
MAKHALIDWE:
SABIC EPDM 756 idapangidwira: kutulutsa kosalala komanso kwachangu, kusakanikirana bwino, kagwiridwe ka mphero ndi mawonekedwe akuthupi, kusungitsa bwino mafuta komanso kuphuka bwino kwamachiritso mumagulu, kudzaza kwambiri.
KUSINTHA NDIKUGWIRITSA NTCHITO:
SABIC EPDM 756 iyenera kusungidwa muzonyamula zake zoyambirira pa kutentha kozungulira mumikhalidwe youma; Kuthamanga kwa pellets kumatha kusokonezedwa ndi kukakamizidwa kapena kutentha kwambiri; kukhudzana ndi kutentha, kuwala kwa ultraviolet ndi kuwala kwa dzuwa kuyenera kupewedwa. Pansi pa malo oyenera osungira, mankhwalawa amakhala okhazikika kwa miyezi 24 kuyambira tsiku lopangidwa. SABIC sidzakulitsa chitsimikiziro chake ngati zinthu zosungira sizikukwanira zomwe zingayambitse kuwonongeka kwabwino monga kuuma kwa pellet kapena kusintha kwamtundu komwe kungapangitse kuti zinthu zisamayende bwino.
Chodzikanira:
Kugulitsa kulikonse ndi SABIC, mabungwe ake ndi othandizana nawo (aliyense 'wogulitsa'), amapangidwa motsatizana ndi zomwe wogulitsa amagulitsa (zopezeka popempha) pokhapokha atagwirizana mwanjira ina ndikusainira m'malo mwa wogulitsa. Ngakhale zomwe zili m'nkhaniyi zaperekedwa mwachikhulupiriro, WOGULITSA SAPANGIZA CHITIDIKIZO, KUTANTHAUZIRA KAPENA ZOCHITA, KUphatikizirapo malonda ndi osalakwira katundu waluntha, KAPENA AMALINGALIRA ULIWONSE, WONSE KAPENA MWACHITATU, PAMODZI NDI MTIMA WONSE, KUGWIRITSA NTCHITO KAPENA CHOLINGA CHA ZINTHU IZI PA NTCHITO ILIYONSE. Makasitomala aliyense ayenera kudziwa kuyenera kwa zinthu zogulitsa kuti agwiritse ntchito makamaka poyesa ndi kusanthula koyenera. Palibe mawu operekedwa ndi wogulitsa okhudzana ndi kugwiritsa ntchito chinthu chilichonse, ntchito kapena kapangidwe kake kamene kamalingaliridwa, kapena kuyenera kutanthauziridwa, kupereka chilolezo pansi pa patent kapena ufulu wina waukadaulo.