SABIC® EPDM 756

SABIC EPDM 756 e maualuga le viscosity mooney, maualuga ethylene ma ENB tulaga tulaga maualuga e gaosia e le
polymerization fofo e faaaoga ai metallocene catalyst. O lo'o i ai le tufatufaina o le mamafa mole mole. E maua lenei oloa ile pellet
fomu.
SABIC EPDM 756 e mafai ona fa'aoga mo: fa'agaioiga fa'apisinisi, fa'agaau ta'avale ma fusipa'u, fa'amatalaga fa'asalalauina, fa'amaufa'ailoga tau ta'avale, fa'aoga e fa'asa'o le vevela
  • 756

  • SABIC

  • SABIC EPDM 756

Avanoa:
Aofa'i:

TULAGA FA'AVAE FA'AVAE:

MEATOAGA TULAGA FAAVAE UNITS METOGA SU'E
MEATOAGA POLIMERA


Ole viscosity ole Mooney


ML 1+4, 125 °C (1) 72
MU
ASTMD 1646
Ethylene Content 69
wt.%
ASTMD 3900
Ethylidene Norbornene (ENB). 5
wt.% ASTMD 6047

UIGA:

 SABIC EPDM 756 ua fuafuaina mo: lamolemole ma vave extrusion, faaleleia fefiloi, mill taulimaina ma meatotino faaletino, lelei le faatumauina o suauu ma faaleleia fofo fuga i totonu o tuufaatasiga, faatumu maualuga utaina.

 TE'U MA TAU'INA:

 SABIC EPDM 756 e tatau ona teuina i totonu o lona uluai afifiina ile vevela vevela ile tulaga mago; e mafai ona a'afia le lelei o pellet i le mamafa po'o le maualuga o le vevela; e tatau ona 'alofia le fa'aalia i le vevela, moli ultraviolet ma le malamalama sa'o o le la. I lalo o tulaga talafeagai e teu ai, o le oloa e mautu mo le 24 masina mai le aso na gaosia ai. Ole SABIC ole a le fa'aopopoina lana saisai pe a le lava le teuina o tulaga e ono i'u ai i le fa'aleagaina lelei e pei ole fa'ama'a'a pellet po'o suiga lanu e ono i'u ai i le le atoatoa o le fa'atinoga o oloa.

 FA'AVAE:

 So'o se fa'atauga a le SABIC, ona lala ma fa'alāpotopotoga (ta'ito'atasi o le 'fa'atau'), e faia fa'apitoa i lalo o tu'utu'uga masani a le fa'atau atu (avanoa pe a talosaga) se'i vagana ua malilie i ai i se faiga tusitusia ma sainia e fai ma sui o le fa'atau. E ui o faʻamatalaga o loʻo i totonu o loʻo tuʻuina atu ma le faʻamaoni, E LE FAIA E LE FAʻAALIGA, FAʻAALIGA PE FAʻAALIGA, E AOFIA AI FAIGA FAʻATAʻAI MA LE LE SULIAINA O METOTIA FAATAMAI, MA LE FAʻAALIGA SOʻO se noataga, tuusaʻo pe le tuusaʻo, e tusa ai ma le faʻaogaina o le faʻatinoga, e tusa ai ma le faʻatinoga, FAAMOEMOEGA O NEI Oloa I SO'O SE TA'IGA. E tatau i tagata fa'atau ta'ito'atasi ona fuafua le talafeagai o mea fa'atau atu mo le fa'aoga patino a le tagata fa'atau e ala i su'ega talafeagai ma au'ili'iliga. E leai se fa'amatalaga a le tagata fa'atau e uiga i le fa'aogaina o so'o se oloa, auaunaga po'o se mamanu ua fa'amoemoe, pe tatau ona faauigaina, e tu'uina atu so'o se laisene i lalo o so'o se pateni po'o isi aia tatau tau le atamai.


Muamua: 
Sosoo ai: 

SO'OGA VAIVAI

OA TATOU Oloa

FA'AALIGA FESOASOANI

Faʻaopoopo: Nu.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Telefoni / WhatsApp / Skype: +86 15221953351
Puletaofia     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |   Faiga Fa'alilolilo | Lagolago e Leadong.