SABIC® EPDM 756

SABIC EPDM 756 yog lub siab mooney viscosity, siab ethylene thiab nruab nrab ENB cov ntsiab lus qib uas tsim los ntawm cov tshuaj
polymerization siv metallocene catalyst. Nws muaj qhov nruab nrab molecular hnyav faib. Cov khoom no muaj nyob rau hauv pellet
daim ntawv.
SABIC EPDM 756 tuaj yeem siv rau: muaj hoses, tsheb hoses thiab siv, extruded profiles, nws pib huab cua ntsaws ruaj ruaj, tshav kub resistant daim ntaub ntawv
  • 756

  • SABIC

  • SAB 756

Muaj:
Quantity:

TSEEM CEEB TSHAJ PLAWS:

PROPERTIES TYPICAL VALUES UNITS KEV TIV THAIV
POLYMER PROPERTIES


Mooney viscosity


ML 1 + 4, 125 ° C (1) 72
MU
TIAB SA 1646
Ethylene Cov ntsiab lus 69
wt.%
ASTM 3900 TSO
Ethylidene Norbornene (ENB) Cov ntsiab lus 5
wt.% TIAB SA 6047

CHARACTERISTIS:

 SABIC EPDM 756 yog tsim los rau: du thiab ceev extrusion, txhim kho kev sib tov, zeb tuav thiab lub cev muaj zog, zoo heev roj tuav thiab txhim kho kev tawg paj hauv cov tebchaw, siab muab tub lim loadable.

 KHOOM thiab kev tuav:

 SABIC EPDM 756 yuav tsum muab khaws cia rau hauv nws qhov qub ntim ntawm ambient kub nyob rau hauv qhuav tej yam kev mob; flowability ntawm cov pellets tuaj yeem cuam tshuam tsis zoo los ntawm kev kub siab lossis kub siab; yuav tsum tsis txhob raug tshav kub, ultraviolet lub teeb thiab ncaj qha tshav ntuj. Raws li qhov tsim nyog khaws cia, cov khoom lag luam ruaj khov rau 24 lub hlis txij li hnub tsim khoom. SABIC yuav tsis txuas ntxiv nws qhov kev lees paub thaum lub sijhawm khaws cia tsis txaus uas yuav ua rau muaj kev puas tsuaj zoo xws li pellet hardening lossis hloov xim uas tuaj yeem ua rau cov khoom lag luam tsis txaus.

 DISCLAIMER:

 Ib qho kev muag khoom los ntawm SABIC, nws cov chaw muag khoom thiab cov koom nrog (txhua tus 'muag'), yog tsim tshwj xeeb raws li tus neeg muag khoom tus qauv kev muag khoom (muaj raws li qhov kev thov) tshwj tsis yog pom zoo ua lwm yam hauv kev sau ntawv thiab kos npe sawv cev ntawm tus neeg muag khoom. Txawm hais tias cov ntaub ntawv muaj nyob rau hauv no tau muab rau hauv kev ntseeg zoo, tus neeg muag khoom tsis muaj kev lav phib xaub, nthuav tawm lossis hais qhia, suav nrog kev muag khoom thiab tsis muaj kev cuam tshuam ntawm kev txawj ntse, lossis tsis muaj kev lav phib xaub, ncaj qha lossis kev cuam tshuam, cuam tshuam, LUB TSEV KAWM NTAWV YUAV TSUM siv los yog lub hom phiaj ntawm cov khoom no hauv txhua daim ntawv thov. Txhua tus neeg siv khoom yuav tsum txiav txim siab qhov tsim nyog ntawm cov ntaub ntawv muag khoom rau cov neeg siv khoom tshwj xeeb los ntawm kev sim thiab tshuaj xyuas tsim nyog. Tsis muaj nqe lus los ntawm tus neeg muag khoom hais txog kev siv tau ntawm txhua yam khoom, kev pabcuam lossis kev tsim qauv, lossis yuav tsum tau txhais, kom muab ib daim ntawv tso cai raws li patent lossis lwm txoj cai kev txawj ntse.


Yav dhau los: 
Tom ntej: 

QUICK LINKS

Peb cov khoom

Tiv tauj xov xwm

Ntxiv: No.33, Txoj Kev 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Copyright ©     2023 Shanghai Herchy Rubber Co., Ltd. Daim duab qhia chaw |   Txoj Cai Tswjfwm Ntiag Tug | Txhawb nqa By Leadong.