SABIC® EPDM 756

SABIC EPDM 756 ke mooney viscosity e phahameng, ethylene e phahameng le boemo bo bohareng ba ENB bo hlahisoang ke tharollo ea
polymerization ho sebelisa metallocene catalyst. E na le kabo ea boima ba molek'hule e mahareng. Sehlahisoa sena se fumaneha ka pellet
sebopeho.
SABIC EPDM 756 e ka sebelisoa bakeng sa: li-hose tsa indasteri, li-hose tsa likoloi le mabanta, li-profile tse fetisitsoeng, litiiso tsa boemo ba leholimo ba likoloi, lisebelisoa tse thibelang mocheso
  • 756

  • SABIC

  • SABIC EPDM 756

Ho fumaneha:
Bongata:

TLHOKOMELISO EA MOSEBETSI:

LETLOTLO LIEKETSENG TS'OANE LIEKETSENG LIEKETSENG MEKHOA
POLYMERE LETLOTLO


Mooney viscosity


ML 1+4, 125 °C (1) 72
MU
Setšoantšo sa ASTMD 1646
Litaba tsa Ethylene 69
wt.%
ASTMD 3900
Ethylidene Norbornene (ENB) Content 5
wt.% ASTMD 6047

LITŠOANTŠISO:

 SABIC EPDM 756 e etselitsoe: extrusion e boreleli le e potlakileng, ho kopanya ho ntlafalitsoeng, ho ts'oaroa ha leloala le thepa ea 'mele, ho boloka oli e ntle haholo le palesa e ntlafalitsoeng ea pheko ka har'a metsoako, ho tlatsa li-filler tse ngata.

 POLOKO LE TŠOARO:

 SABIC EPDM 756 e lokela ho bolokoa ka har'a sephutheloana sa eona sa pele mochesong o omileng maemong a omileng; phallo ea li-pellets e ka susumetsoa hampe ke khatello kapa mocheso o phahameng; ho pepesehela mocheso, khanya ea ultraviolet le khanya ea letsatsi e tobileng e lokela ho qojoa. Tlas'a maemo a loketseng a polokelo, sehlahisoa se tsitsitse likhoeli tse 24 ho tloha letsatsing la tlhahiso. SABIC e ke ke ea atolosa tiisetso ea eona ha maemo a polokelo a sa lekana a ka lebisang ho senyeha ha boleng bo kang ho thatafala ha pellet kapa ho fetoha ha 'mala ho ka bakang ts'ebetso e sa lekaneng ea sehlahisoa.

 TLHOKOMELO:

 Thekiso efe kapa efe e entsoeng ke SABIC, litsi tsa eona le mekhatlo e amanang le eona (e 'ngoe le e 'ngoe e le 'morekisi'), e etsoa ka mokhoa o ikhethileng tlas'a maemo a tloaelehileng a thekiso (a fumaneha ka kopo) ntle le haeba ho lumellanoe ka mokhoa o mong ka lengolo le ho saenoa molemong oa morekisi. Leha tlhahisoleseling e fanoeng mona e fanoe ka tumelo e ntle, morekisi HA A SEBELE TIISETSO, HO BONAHALA KAPA HO FIHLELANG, HO kenyeletsoa THEKISO LE HO HLOKA TLOELO EA TLHOKOMELISO EA MAHLALE, HONA HA A HLAHALA MORATO OFE KA FEELA KAPA HO HLOKA BOHLOKO, KA HLOMPHO, TŠEBELETSO KAPA MORERO OA LIHLAHISO TSENA HO KOPO EFE KA EFE. Moreki e mong le e mong o tlameha ho etsa qeto ea ho tšoaneleha ha lisebelisoa tsa morekisi bakeng sa tšebeliso e khethehileng ea moreki ka tlhahlobo le tlhahlobo e nepahetseng. Ha ho polelo ea morekisi mabapi le tšebeliso e ka bang teng ea sehlahisoa, tšebeletso kapa moralo o reretsoeng, kapa o lokelang ho hlalosoa, ho fana ka laesense efe kapa efe tlasa tokelo efe kapa efe ea tokelo ea molao kapa tokelo e 'ngoe ea thepa ea mahlale.


E fetileng: 
E 'ngoe: 

LIEKETSENG POTLAKO

LIHLAHISO TSA RONA

MOKHOA OA PUISANO

Eketsa: No.33, Lane 159, Taiye Road, Setereke sa Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Sebaka sa marang-rang |   Leano la Lekunutu | Tšehetso Ka Leadong.