756
SABIC
Farashin EPDM756
| Samuwar: | |
|---|---|
| Yawan: | |
DARAJAR ARZIKI NA DUKIYA:
| DUKIYA | MATSALOLIN MATAKI | RAKA'A | HANYOYIN gwaji |
| KAYAN POLYMER | |||
| Dankowar Mooney | |||
| ML 1+4, 125 °C (1) | 72 |
MU |
Saukewa: ASTMD1646 |
| Abubuwan Ethylene | 69 |
wt.% |
Saukewa: ASTMD3900 |
| Abun ciki Ethylidene Norbornene (ENB). | 5 |
wt.% | Saukewa: ASTMD6047 |
HALAYE:
SABIC EPDM 756 an tsara shi don: santsi da sauri extrusion, ingantaccen haɗawa, sarrafa niƙa da kaddarorin jiki, kyakkyawan riƙewar mai da ingantaccen fure mai fure a cikin mahadi, babban filler mai ɗaukar nauyi.
ARZIKI DA MULKI:
SAIC EPDM 756 yakamata a adana shi a cikin ainihin marufi a yanayin zafi a yanayin bushewa; gudanawar pellets na iya zama mummunan tasiri ta matsa lamba ko babban zafin jiki; ya kamata a guje wa fuskantar zafi, hasken ultraviolet da hasken rana kai tsaye. A ƙarƙashin yanayin ajiyar da ya dace, samfurin ya tsaya tsayin daka na tsawon watanni 24 daga ranar da aka yi. SABIC ba za ta tsawaita garantin sa ba lokacin da yanayin ajiya bai isa ba wanda zai iya haifar da lalacewa mai inganci kamar taurin pellet ko canjin launi wanda zai iya haifar da ƙarancin aikin samfur.
RA'AYI:
Duk wani tallace-tallace ta SABIC, rassan sa da masu haɗin gwiwa (kowane mai siyarwa), ana yin shi ne kawai a ƙarƙashin daidaitattun sharuɗɗan siyarwa