SABIC® EPDM 756

SABIC EPDM 756 ndeye high mooney viscosity, yakakwira ethylene uye yepakati ENB yemukati giredhi inogadzirwa nemhinduro
polymerization uchishandisa metallocene catalyst. Iine medium molecular weight distribution. Ichi chigadzirwa chinowanikwa mupellet
form.
SABIC EPDM 756 inogona kushandiswa ku: hosi dzemaindasitiri, hosi dzemotokari nemabhandi, maprofiles akawedzerwa, zvisimbiso zvemamiriro ekunze emotokari, zvisimbiso zvinodzivirira kupisa
  • 756

  • SABIC

  • SABIC EPDM 756

Kuwanikwa:
Huwandu:

TYPICAL PROPERTY VALUES:

PROPERTIES ZVINOKOSHA ZVAKAWANDA UNITS DZIDZO NZIRA
POLYMER PROPERTIES


Mooney viscosity


ML 1+4, 125 °C (1) 72
MU
ASTMD 1646
Ethylene Content 69
wt.%
ASTMD 3900
Ethylidene Norbornene (ENB) Zviri mukati 5
wt.% ASTMD 6047

ZVINHU:

 SABIC EPDM 756 yakagadzirirwa: yakatsetseka uye inokurumidza extrusion, yakagadziridzwa musanganiswa, mabatiro eguyo uye emuviri zvimiro, yakanakisa kuchengetedza mafuta uye yakagadziridzwa kurapa inotumbuka mumakomponi, yakakwira mafirita anotakurika.

 KUCHENGETA UYE KUBATA:

 SABIC EPDM 756 inofanira kuchengetwa mukutakura kwayo kwepakutanga pane tembiricha yakadzika mumamiriro akaoma; kuyerera kwepellets kunogona kukanganiswa nekumanikidzwa kana kupisa kwakanyanya; kutarisana nekupisa, ultraviolet chiedza uye chiedza chezuva chakananga chinofanira kudzivirirwa. Pasi pemamiriro ekuchengetedza akakodzera, chigadzirwa chacho chakagadzikana kwemwedzi makumi maviri nemana kubva pazuva rekugadzirwa. SABIC haizowedzeri waranti yayo kana mamiriro ekuchengetera asina kukwana izvo zvinogona kukonzeresa kushata kwemhando sekuomesa pellet kana shanduko yeruvara izvo zvinogona kukonzera kusakwana kwechigadzirwa.

 ZVINOTAURWA:

 Chero kutengeswa neSABIC, vatsigiri vayo uye vanobatana (mumwe nemumwe 'mutengesi'), anoitwa chete pasi pemamiriro ekutengesa akajairwa nemutengesi (anowanikwa pakukumbira) kunze kwekunge kwabvumiranwa neimwe nzira nekunyora uye kusainwa pachinzvimbo chemutengesi. Nepo ruzivo rwuri pano ruchipihwa nekutenda kwakanaka, MUtengesi HAAITA WARRANTI, ZVINOTAURWA KANA ZVINOREVEDZERA, zvinosanganisira KUTENGESEKA UYE KUSANGANISWA KWEZVINHU ZVINOCHENJERERA, KANA KUTAMBURA ZVINHU ZVINHU, ZVINHU ZVINHU KANA KUSIYANA, NERUREMEKO NEKUKATAMIRA, KUSHANDISWA KUSHANDISWA KANA KUNANGWA KWEZVINHU ZVINO MUCHINHU CHESE. Mutengi wega wega anofanirwa kuona kukodzera kwezvinhu zvemutengesi zvekushandiswa kwemutengi kuburikidza nekuyedzwa nekuongorora kwakakodzera. Hapana chirevo chemutengesi chine chekuita nekugona kushandiswa kwechero chigadzirwa, sevhisi kana dhizaini inoitirwa, kana inofanirwa kutsanangurwa, kupa chero rezinesi pasi pechero patent kana imwe kodzero yekuziva.


Zvakapfuura: 
Zvinotevera: 

KUKURUMIDZA ZVINONYANYA

ZVINHU ZEDU

CONTACT INFORMATION

Wedzera: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |   Privacy Policy | Support By Leadong.