SABIC® EPDM 626

SABIC EPDM 626 ndi sing'anga kukhuthala kwa mooney, high ethylene ndi otsika ENB okhutira kalasi opangidwa ndi yankho polymerization ntchito metallocene chothandizira. Ili ndi gawo laling'ono la molekyulu yolemetsa. Izi zimapezeka mu pellet mawonekedwe.
  • 626

  • Mtengo wa magawo SABIC

  • Chithunzi cha SABIC EPDM626

kupezeka:
kuchuluka:

MFUNDO ZOYENERA KUCHITA:

ZINTHU MFUNDO ZOYENERA MALANGIZO NJIRA ZOYESA
ZINTHU ZA POLYMER


Kukhuthala kwa Mooney


ML 1+4, 125 °C (1) 67
MU
Chithunzi cha ASTMD 1646
Zinthu za Ethylene 69
wt.%
Mtengo wa ASMD3900
Ethylidene Norbornene (ENB) Zomwe zili 2.8
wt.% Chithunzi cha ASTMD6047

MAKHALIDWE:

 SABIC EPDM 626 idapangidwa kuti ikhale: zinthu zabwino zakuthupi, kusakanikirana bwino ndi kagwiridwe ka mphero, kuwongolera bwino, kusunga bwino kwamafuta, kuchepetsedwa kwamachiritso pachimake mumagulu.

KUSINTHA NDI KUGWIRITSA NTCHITO: SABIC EPDM 626 iyenera kusungidwa muzonyamula zake zoyambirira pa kutentha kozungulira mumikhalidwe youma; Kuthamanga kwa pellets kumatha kusokonezedwa ndi kukakamizidwa kapena kutentha kwambiri; kukhudzana ndi kutentha, kuwala kwa ultraviolet ndi kuwala kwa dzuwa kuyenera kupewedwa. Pansi pa malo oyenera osungira, mankhwalawa amakhala okhazikika kwa miyezi 24 kuyambira tsiku lopangidwa. SABIC sidzakulitsa chitsimikiziro chake ngati zinthu zosungira sizikukwanira zomwe zingayambitse kuwonongeka kwabwino monga kuuma kwa pellet kapena kusintha kwamtundu komwe kungapangitse kuti zinthu zisamayende bwino.

 ZOYENERA Kugulitsa kulikonse ndi SABIC, mabungwe ake ndi othandizana nawo (aliyense 'wogulitsa'), amapangidwa motsatizana ndi zomwe wogulitsa amagulitsa (zopezeka popempha) pokhapokha atagwirizana mwanjira ina ndikusainira m'malo mwa wogulitsa. Ngakhale zomwe zili m'nkhaniyi zaperekedwa mwachikhulupiriro, WOGULITSA SAPANGIZA CHITIDIKIZO, KUTANTHAUZIRA KAPENA ZOCHITA, KUphatikizirapo malonda ndi osalakwira katundu waluntha, KAPENA AMALINGALIRA ULIWONSE, WONSE KAPENA MWACHITATU, PAMODZI NDI MTIMA WONSE, KUGWIRITSA NTCHITO KAPENA CHOLINGA CHA ZINTHU IZI PA NTCHITO ILIYONSE. Makasitomala aliyense ayenera kudziwa kuyenera kwa zinthu zogulitsa kuti agwiritse ntchito makamaka poyesa ndi kusanthula koyenera. Palibe mawu operekedwa ndi wogulitsa okhudzana ndi kugwiritsa ntchito chinthu chilichonse, ntchito kapena kapangidwe kake kamene kamalingaliridwa, kapena kuyenera kutanthauziridwa, kupereka chilolezo pansi pa patent kapena ufulu wina waukadaulo.


Zam'mbuyo: 
Ena: 

MALANGIZO OPHUNZITSA

ZOPHUNZITSA ZATHU

ZAMBIRI ZAMALUMIKIZIDWE

Onjezani: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Ufulu     2023 Shanghai Herchy Rubber Co., Ltd. Mapu atsamba |   Mfundo Zazinsinsi | Support By Leadong.