Product Overview: Oil chakna sang tak nei, medium-Saturation HNBR Synthetic Rubber
Kan Medium-Saturation HNBR Synthetic Rubber hi oil-exposed leh high-stress industrial environment-a performance danglam tak pe thei tura engineer a ni. 34% acrylonitrile content neiin, he hydrogenated nitrile rubber (HNBR) hian oil resistance tha zawk a pe a, chutih rualin flexibility leh durability a vawng reng a, hei hian seal, gasket, leh components te tan pawh a tha hle a, hnathawhna hmun harsa takah pawh a tha hle.
Technical lam thil pawimawh tak takte:
- Acrylonitrile Content: 34% – Oil resistance balanced leh low-temperature flexibility atan a tha ber.
- Mooney Viscosity (ML 1+4 @125°C): 70-90 – Moulding leh extrusion atan processability tha tak a siam.
- Iodine Absorption Value: 11-22 – Chemical stability tihchangtlunna tur leh tar chak lohna tur controlled medium saturation a lantir.
- Hardness: Application hrang hrang mamawh phuhruk nan range (eg, 60-90 Shore A) siamrem theih.
Performance lama thatna: 1.1.
- Superior Oil & Fuel Resistance: Oil, grease, leh hydrocarbon fluid (ASTM D471 anga test) te nena rei tak a awm chuan a tuar thei.
- High Tensile Strength: Dynamic load leh pressure nasa tak hnuaiah structural integrity a vawng reng thin.
- Thermal Stability: -30°C atanga +150°C (-22°F atanga +302°F) inkar ah rintlak takin a thawk thei.
- Abrasion Resistance: Rotating seal leh hydraulic system ang chi high-wear application atan a tha hle.
Dilna: 1.1.
- Oil & Gas: Pump, valve, leh downhole hmanrua te seal.
- Automotive: Fuel system components, O-rings, leh timing belts te a awm a.
- Industrial Machinery: Chemical processing atana hman tur gasket, hose, leh custom-molded parts te.
Engvangin Nge Kan HNBR Hi Kan Thlan?
- Customizable Formulations: Hardness, viscosity, leh saturation level te chu mamawh bik atan siamin.
- Quality inmil: ISO 9001 leh ASTM standard nena inmil.
- Extended Service Life: Oil awmna hmun pawimawh takah downtime a ti tlem.